Kurz gefasst

Fachartikel in der Zeitschrift Ceramics, online erschienen am 06.11.2026. Verfasst von Aizat Bakytkyzy und 7 weiteren Autor:innen. Die Arbeit nennt 82 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

The photoluminescence (PL) and photoluminescence excitation (PLE) spectra of an EFG-grown (−201) β-Ga2O3 single crystal were recorded at 7 and 300 K at the FinEstBeAMS beamline of the MAX IV Laboratory. Excitation–emission maps and fixed-wavelength PLE profiles covered 4.50–10.50 eV at both temperatures. Each temperature series was normalized to its own 5.00 eV intensity and, alternatively, to its own maximum; the reported ratios therefore describe excitation dependence within one series and not an absolute difference in luminescence yield between temperatures. At 7 K, integrated emission at 10.50 eV retains 95.4% of its 5.00 eV value and 89.2% of its maximum. At 300 K, the PLE half-height is 4.55 eV, and the maximum occurs at 4.75–4.80 eV, followed by a decrease to 2.26% of the 5.00 eV value and 2.03% of the maximum at 10.50 eV. Room-temperature ellipsometry on the same factory-polished face places the PLE rise in the rapidly increasing absorption region and yields a penetration depth of approximately 0.24 μm near the PLE half-height and 37 nm at 5.90 eV. A constrained depth-dependent calculation does not reproduce the full decline, so surface capture is retained as one possible pathway rather than an established mechanism. The emission is described by the same effective bands at 3.55, 3.37 and 3.07 eV used in the preceding laser study. Their balance is nearly constant at 7 K, whereas the low-energy spectral weight increases at 300 K under deep-VUV excitation. These spectra provide quantitative reference profiles for energy conversion and carrier capture in β-Ga2O3.

Zitieren

APA

Bakytkyzy, A., Karipbayev, Z. T., Zhurkin, E. B., Akhmetova-Abdik, G. A., Konuhova, M., Zhunusbekov, A. M., Chernenko, K., & Popov, A. I. (2026). UV–VUV Excitation Profiles of Luminescence in β-Ga2O3 Single Crystals. Ceramics, 9(11), 127. https://doi.org/10.3390/ceramics9110127

Vancouver

Bakytkyzy A, Karipbayev ZT, Zhurkin EB, Akhmetova-Abdik GA, Konuhova M, Zhunusbekov AM, et al. UV–VUV Excitation Profiles of Luminescence in β-Ga2O3 Single Crystals. Ceramics. 2026;9(11):127. doi:10.3390/ceramics9110127

BibTeX
@article{Bakytkyzy2026,
  author = {Bakytkyzy, Aizat and Karipbayev, Zhakyp T. and Zhurkin, Ernar B. and Akhmetova-Abdik, Gulzhanat A. and Konuhova, Marina and Zhunusbekov, Amangeldy M. and Chernenko, Kirill and Popov, Anatoli I.},
  title = {UV–VUV Excitation Profiles of Luminescence in β-Ga2O3 Single Crystals},
  journal = {Ceramics},
  year = {2026},
  volume = {9},
  number = {11},
  pages = {127},
  doi = {10.3390/ceramics9110127}
}