EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Two-Step Sintering and Sr(Fe0.5Nb0.5)O3 Addition Enhancing Electrical Properties of KNN-Based Lead-Free Piezoelectric Ceramics

Yafei Miao, Shaohua Su, Bijun Fang, Shuai Zhang, Xiaolong Lu, Jianning Ding

Ceramics · 31.10.2026 · 9 (11) · 123

DOI: 10.3390/ceramics9110123 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Ceramics, online erschienen am 31.10.2026. Verfasst von Yafei Miao und 5 weiteren Autor:innen. Die Arbeit nennt 55 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Lead-free (1−x)(K0.49Na0.51)(Nb0.95Sb0.05)O3-xSr(Fe0.5Nb0.5)O3 [(1−x)KNNbS-xSrFNb, x = 0.01–0.07] ceramics with 0.5 wt% CuO were prepared by conventional sintering (CS) and two-step sintering (TSS). Increasing the SrFNb content drives the structure from orthorhombic–tetragonal (O-T, x ≤ 0.03) coexistence to rhombohedral–tetragonal (R-T, x ≥ 0.05) coexistence, and shifts the phase boundary toward room temperature, while Fe3+/Nb5+ B-site disorder induces polar nanoregions, diffuse dielectric behavior (dispersion index γ > 1.7) and a drop of Tm (temperature of dielectric constant maximum) from 295 °C to below room temperature. Increasing SrFNb significantly reduces the average grain size from 0.6 μm to 0.3 μm, while TSS decouples densification from grain growth, raising the maximum relative density from 92.13% to 94.51% at x = 0.05 with only a slight reduction in average grain size from 0.35 μm to 0.32 μm. These changes directly tailor the electrical properties: the near-room-temperature O-T boundary at x = 0.03 gives the best soft-type response (piezoelectric constant d33 = 133 pC/N, electromechanical coupling coefficient Kp = 0.285, remnant polarization Pr = 22.72 μC/cm2), whereas acceptor-oxygen-vacancy dipoles at x = 0.01 pin domain walls, yielding the highest mechanical quality factor Qm = 329 with low tan δ, and TSS further improves fatigue resistance. Combining SrFNb-driven structural evolution with TSS microstructural control thus offers an effective route to tailor KNN-based lead-free piezoelectrics.

Zitieren

APA

Miao, Y., Su, S., Fang, B., Zhang, S., Lu, X., & Ding, J. (2026). Two-Step Sintering and Sr(Fe0.5Nb0.5)O3 Addition Enhancing Electrical Properties of KNN-Based Lead-Free Piezoelectric Ceramics. Ceramics, 9(11), 123. https://doi.org/10.3390/ceramics9110123

Vancouver

Miao Y, Su S, Fang B, Zhang S, Lu X, Ding J. Two-Step Sintering and Sr(Fe0.5Nb0.5)O3 Addition Enhancing Electrical Properties of KNN-Based Lead-Free Piezoelectric Ceramics. Ceramics. 2026;9(11):123. doi:10.3390/ceramics9110123

BibTeX
@article{Miao2026,
  author = {Miao, Yafei and Su, Shaohua and Fang, Bijun and Zhang, Shuai and Lu, Xiaolong and Ding, Jianning},
  title = {Two-Step Sintering and Sr(Fe0.5Nb0.5)O3 Addition Enhancing Electrical Properties of KNN-Based Lead-Free Piezoelectric Ceramics},
  journal = {Ceramics},
  year = {2026},
  volume = {9},
  number = {11},
  pages = {123},
  doi = {10.3390/ceramics9110123}
}