Fachartikel in der Zeitschrift Catalysts, online erschienen am 23.11.2026. Verfasst von Yu Chen und 8 weiteren Autor:innen. Die Arbeit nennt 43 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Inner Mongolia Autonomous Region Key Research and Development Program.
Abstract (Originalsprache)
The NH3-SCR performance of Fe-Ce-Mn/TiO2 catalysts depends on calcination temperature. To examine this effect at fixed composition, 8Fe2O3-5CeO2-40MnO2/TiO2 was prepared by co-precipitation and calcined at 200, 300, 400 or 500 °C for 4 h. The 400 °C sample provided the widest temperature range with at least 90% NO conversion (129–390 °C), reached a maximum of 99.17% and had the lowest apparent activation energy (55.78 kJ mol−1). It showed favorable N2 selectivity and retained the highest conversion in the SO2 and combined SO2/H2O resistance tests. XRD, N2 physisorption, microscopy, XPS, NH3-TPD and H2-TPR results showed that calcination altered pore development, particle aggregation and surface properties. At lower calcination temperatures, less developed pores and greater aggregation limited the exposure of supported metal species and coincided with poorer SCR performance. By 400 °C, pore development and particle dispersion had improved, accompanied by greater surface metal exposure, NH3 uptake and overall reducibility. Further heating to 500 °C increased aggregation and reduced surface metal fractions and total NH3 uptake without improving activity. Calcination at 400 °C for 4 h gave the best overall performance in the series.
Förderung
- Inner Mongolia Autonomous Region Key Research and Development Program
Zitieren
APA
Chen, Y., Yang, Y., Bian, X., Li, J., Mu, X., Jia, Z., Wang, Z., Zhang, B., & Hong, G. (2026). Effect of Calcination Temperature on the Structure and NH3-SCR Performance of 8Fe2O3-5CeO2-40MnO2/TiO2 Catalysts. Catalysts, 16(12), 1053. https://doi.org/10.3390/catal16121053
Vancouver
Chen Y, Yang Y, Bian X, Li J, Mu X, Jia Z, et al. Effect of Calcination Temperature on the Structure and NH3-SCR Performance of 8Fe2O3-5CeO2-40MnO2/TiO2 Catalysts. Catalysts. 2026;16(12):1053. doi:10.3390/catal16121053
BibTeX
@article{Chen2026,
author = {Chen, Yu and Yang, Yuming and Bian, Xue and Li, Jiaqi and Mu, Xuewen and Jia, Zhongshuai and Wang, Zhicheng and Zhang, Bin and Hong, Guomin},
title = {Effect of Calcination Temperature on the Structure and NH3-SCR Performance of 8Fe2O3-5CeO2-40MnO2/TiO2 Catalysts},
journal = {Catalysts},
year = {2026},
volume = {16},
number = {12},
pages = {1053},
doi = {10.3390/catal16121053}
}
EUVIMED