EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Residual Mechanical Performance and Mass Loss of Heat-Cured NaOH-Activated Fly Ash/Slag and Portland Cement Mortars After Exposure to Elevated Temperatures

Erion Luga, Enea Mustafaraj, Marco Corradi, Ela Görür Avşaroğlu, Cengiz Duran Atiş

Buildings · 09.11.2026 · 16 (21) · 4469

DOI: 10.3390/buildings16214469 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Buildings, online erschienen am 09.11.2026. Verfasst von Erion Luga und 4 weiteren Autor:innen. Die Arbeit nennt 31 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

This study compares the residual mechanical performance and mass loss of NaOH-activated Fly Ash (FA), Ground Granulated Blast Furnace Slag (GGBFS) and FA/GGBFS mortars with those of CEM I 42.5R and CEM I 52.5R mortars after exposure to 300, 600 and 900 °C. The alkali-activated mortars were heat-cured at 100 °C for 3 days, whereas the Ordinary Portland Cement (OPC) mortars were water-cured for 28 days, to compare the residual performance of the materials produced under their respective curing regimes. After 900 °C, the GGBFS mortar retained 43.4 MPa in compression (57.5%) and 2.88 MPa in flexure (44.9%), against 6.4–9.1 MPa (11.7–14.6%) and 1.29–1.40 MPa (12.8–16.3%) for the OPC mortars, both differences being statistically significant for each OPC mortar. The FA/GGBFS mortar (33.9 MPa, 50.9% in compression) exceeded the OPC mortars only in mean value; the differences were not statistically significant. GGBFS showed the highest mass loss (7.83% at 900 °C). In a correlation analysis, mass loss mirrored strength loss in the OPC mortars (R2 = 0.92–0.98) but not in the alkali-activated ones (R2 ≤ 0.11), showing that mass loss alone was not a consistent indicator of thermal damage across binder systems. The results indicate that the GGBFS-based NaOH-activated mortar is a promising alternative to OPC for precast building elements that must retain residual load-bearing capacity after high-temperature exposure.

Zitieren

APA

Luga, E., Mustafaraj, E., Corradi, M., Avşaroğlu, E. G., & Atiş, C. D. (2026). Residual Mechanical Performance and Mass Loss of Heat-Cured NaOH-Activated Fly Ash/Slag and Portland Cement Mortars After Exposure to Elevated Temperatures. Buildings, 16(21), 4469. https://doi.org/10.3390/buildings16214469

Vancouver

Luga E, Mustafaraj E, Corradi M, Avşaroğlu EG, Atiş CD. Residual Mechanical Performance and Mass Loss of Heat-Cured NaOH-Activated Fly Ash/Slag and Portland Cement Mortars After Exposure to Elevated Temperatures. Buildings. 2026;16(21):4469. doi:10.3390/buildings16214469

BibTeX
@article{Luga2026,
  author = {Luga, Erion and Mustafaraj, Enea and Corradi, Marco and Avşaroğlu, Ela Görür and Atiş, Cengiz Duran},
  title = {Residual Mechanical Performance and Mass Loss of Heat-Cured NaOH-Activated Fly Ash/Slag and Portland Cement Mortars After Exposure to Elevated Temperatures},
  journal = {Buildings},
  year = {2026},
  volume = {16},
  number = {21},
  pages = {4469},
  doi = {10.3390/buildings16214469}
}
Kostenlos starten →