EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Freeze–Thaw Performance and Microstructural Stability of Alkali-Activated Slag Mortars Incorporating Mussel Shell Waste

Merve Şahin Yön

Buildings · 24.06.2026 · 16 (13) · 2511

DOI: 10.3390/buildings16132511 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Buildings, online erschienen am 24.06.2026. Verfasst von Merve Şahin Yön. Die Arbeit nennt 83 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

This study investigates the use of mussel shells (MSs), a biogenic by-product of the food industry, as a partial replacement for ground granulated blast furnace slag (GBFS) in alkali-activated mortars. Given their high CaCO3 content, MSs represent a sustainable secondary raw material that reduces both waste disposal burden and reliance on natural resources, while offering a low-carbon alternative to conventional cement-based binders. Alkali-activated mussel shell/slag mortars (AAMSs) were produced with MS replacement ratios of 0%, 5%, 10%, 15%, and 20% by mass of GBFS. Sodium hydroxide (NaOH) and sodium silicate (Na2SiO3) were used as alkaline activators. Fresh specimens were cured at 60 °C for 48 h. The experimental program included workability, compressive and flexural strength, water absorption, porosity, density, capillarity, ultrasonic pulse velocity (UPV), and freeze–thaw (F-T) resistance tests. Increasing MS content slightly reduced flowability and mechanical strength, while increasing water absorption, porosity, and capillarity. The M0 series achieved the highest 28-day compressive strength (54.06 MPa), while M15 exhibited the highest flexural strength (5.23 MPa). Following F-T cycling, the 5% and 10% MS series demonstrated the best compressive strength (30 MPa). The 10% MS exhibits a relatively balanced overall performance, providing the best balance between mechanical performance, F-T resistance, and microstructural stability, as confirmed by scanning electron microscopy (SEM)/energy-dispersive X-ray spectroscopy (EDS) analyses showing elevated Ca/Si ratios and the formation of Ca-rich crystalline phases.

Zitieren

APA

Yön, M. Ş. (2026). Freeze–Thaw Performance and Microstructural Stability of Alkali-Activated Slag Mortars Incorporating Mussel Shell Waste. Buildings, 16(13), 2511. https://doi.org/10.3390/buildings16132511

Vancouver

Yön MŞ. Freeze–Thaw Performance and Microstructural Stability of Alkali-Activated Slag Mortars Incorporating Mussel Shell Waste. Buildings. 2026;16(13):2511. doi:10.3390/buildings16132511

BibTeX
@article{Yn2026,
  author = {Yön, Merve Şahin},
  title = {Freeze–Thaw Performance and Microstructural Stability of Alkali-Activated Slag Mortars Incorporating Mussel Shell Waste},
  journal = {Buildings},
  year = {2026},
  volume = {16},
  number = {13},
  pages = {2511},
  doi = {10.3390/buildings16132511}
}
Kostenlos starten →