Towards Sustainable Mortar: Optimising Sika-Fibre Dosage in Ground Granulated Blast Furnace Slag (GGBS) and Silica Fume Blends for 3D Concrete Printing
Buildings · 23.09.2025 · 15 (19) · 3436
DOI: 10.3390/buildings15193436 ↗Kurz gefasst
Fachartikel in der Zeitschrift Buildings, online erschienen am 23.09.2025. Verfasst von Wen Si und 3 weiteren Autor:innen. Die Arbeit wurde bisher 15-mal zitiert (Crossref) und nennt 72 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Construct Innovate Technology Centre and Harcourt Technologies Limited (HTL), Ecocem Materials.
Abstract (Originalsprache)
Three-dimensional concrete printing (3DCP) is rapidly emerging as a transformative construction technology, enabling formwork-free fabrication, geometric flexibility, and reduced labour. However, the lack of conventional reinforcement and the strict requirements for fresh and hardened properties present significant challenges. Fibre reinforcement and supplementary cementitious materials (SCMs), such as ground granulated blast furnace slag (GGBS), offer pathways to enhance printability while mitigating environmental impact. This study investigates the combined effect of natural cellulose microfibres and silica fume on the rheological, mechanical, and sustainability performance of 3D-printable mortars. Six mixes were prepared with 50% GGBS, 45% cement, and 5% silica fume, incorporating fibre dosages from 0% to 1%. Results showed that a 0.5% fibre dosage provided the most favourable balance. At this dosage, static yield stress increased to 9.35 Pa and thixotropy reached 8623 mPa·s, enhancing structuration for shape retention. Plastic viscosity remained stable at 4–5 Pa·s, ensuring adequate extrusion performance. Higher fibre dosages (≥0.75%) caused a significant increase in rheological resistance, with static yield stress reaching 208 Pa and thixotropy 135,342 mPa·s. This resulted in excessive structuration, fibre clustering, and poor extrudability. Compressive strength was achieved at 109.10 MPa (92% of silica fume-only mix) with 0.5% fibre. In comparison, flexural strength was 13.20 MPa at 0.5% fibre content and reduced gradually to 12.29 MPa at 1% fibre due to weak fibre–matrix bonding and porosity. Sustainability analysis confirmed that using 50% GGBS and 5% silica fume reduced embodied carbon compared to a 100% cement mix. This study also demonstrated that cellulose microfibres at 0.25–0.5% are optimal for balancing fresh properties, mechanical strength, and sustainability in 3D-printed mortars.
Förderung
- Construct Innovate Technology Centre and Harcourt Technologies Limited (HTL)
- Ecocem Materials
Zitieren
APA
Si, W., Hopkins, B., Khan, M., & McNally, C. (2025). Towards Sustainable Mortar: Optimising Sika-Fibre Dosage in Ground Granulated Blast Furnace Slag (GGBS) and Silica Fume Blends for 3D Concrete Printing. Buildings, 15(19), 3436. https://doi.org/10.3390/buildings15193436
Vancouver
Si W, Hopkins B, Khan M, McNally C. Towards Sustainable Mortar: Optimising Sika-Fibre Dosage in Ground Granulated Blast Furnace Slag (GGBS) and Silica Fume Blends for 3D Concrete Printing. Buildings. 2025;15(19):3436. doi:10.3390/buildings15193436
BibTeX
@article{Si2025,
author = {Si, Wen and Hopkins, Ben and Khan, Mehran and McNally, Ciaran},
title = {Towards Sustainable Mortar: Optimising Sika-Fibre Dosage in Ground Granulated Blast Furnace Slag (GGBS) and Silica Fume Blends for 3D Concrete Printing},
journal = {Buildings},
year = {2025},
volume = {15},
number = {19},
pages = {3436},
doi = {10.3390/buildings15193436}
}
EUVIMED