Fachartikel in der Zeitschrift Buildings, online erschienen am 30.04.2025. Verfasst von Jianguang Xu und 9 weiteren Autor:innen. Die Arbeit wurde bisher 9-mal zitiert (Crossref) und nennt 57 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: National Key Research and Development Project.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

To enhance the microstructure and mechanical properties and to optimize the formulations of high-strength and high-flow ultra-high-performance concrete (UHPC), the effects of different quartz powder contents, fineness, and curing temperatures of UHPC were systematically studied. It was hypothesized that using the appropriate content and fineness of quartz powder can improve the microstructure of UHPC and, thus, improve its mechanical properties, especially at higher curing temperatures. To test this hypothesis, the flowability, compressive strength, flexural strength, and tensile strength of UHPC mixtures with different quartz powder dosages (0%, 15%, 30%) and fineness (4 µm, 8 µm), cured at 20 °C, 45 °C, and 90 °C, were investigated. The results indicate that as the dosage of quartz powder increases and the particle size decreases, the flowability of UHPC decreases. The compressive strength of UHPC first increases and then decreases with an increase in quartz powder dosage. Finer quartz powder usage considerably enhances packing density and pore structure. When the content of quartz powder is 15%, UHPC achieves optimal mechanical properties and pore structure, showing an improvement of 3.6% to 14.4% compared to UHPC with a coarse particle size. Additionally, an increase in curing temperature leads to the consistent growth of the compressive strength of UHPC. Under 90 °C steam curing, UHPC incorporating 15% fine quartz powder (4 μm) achieved a peak compressive strength of 182.1 MPa, increased by 19.8% compared to that under 20 °C, which is attributed to the enhanced pozzolanic activity of fine quartz powder. These findings provide valuable guidance for the mix design of UHPC in precast concrete components, long-span bridges, and marine structures, where high early strength and durability are critical.

Förderung

  • National Key Research and Development Project

Zitieren

APA

Xu, J., Li, Y., Huang, Y., Yuan, G., Cao, Z., Zhang, W., Zheng, H., Zang, Y., Mao, X., & Li, M. (2025). Understanding the Role of Quartz Powder Content and Fineness on the Micro-Structure and Mechanical Performance of UHPC. Buildings, 15(9), 1513. https://doi.org/10.3390/buildings15091513

Vancouver

Xu J, Li Y, Huang Y, Yuan G, Cao Z, Zhang W, et al. Understanding the Role of Quartz Powder Content and Fineness on the Micro-Structure and Mechanical Performance of UHPC. Buildings. 2025;15(9):1513. doi:10.3390/buildings15091513

BibTeX
@article{Xu2025,
  author = {Xu, Jianguang and Li, Yongsheng and Huang, Yue and Yuan, Guojian and Cao, Zhonglu and Zhang, Wei and Zheng, Heping and Zang, Yun and Mao, Xingtai and Li, Mengmeng},
  title = {Understanding the Role of Quartz Powder Content and Fineness on the Micro-Structure and Mechanical Performance of UHPC},
  journal = {Buildings},
  year = {2025},
  volume = {15},
  number = {9},
  pages = {1513},
  doi = {10.3390/buildings15091513}
}
Kostenlos starten →