Effects of Sintering Parameters on the Microstructure and Optical Transmittance of Monolithic 4 mol% Yttria-Partially Stabilized Zirconia

Taek-Jun Chung iD, Myung-Joo Kim iD, Ho-Beom Kwon, Bongju Kim iD, Young-Jun Lim iD

Bioengineering · 19.06.2026 · 13 (6) · 702

DOI: 10.3390/bioengineering13060702 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Bioengineering, online erschienen am 19.06.2026. Verfasst von Taek-Jun Chung und 4 weiteren Autor:innen. Beteiligte Einrichtung: Department of Prosthodontics and Dental Research Institute, School of Dentistry, Seoul National University, Seoul 03085, Republic of Korea. Die Arbeit nennt 32 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Seoul National University Dental Hospital, SNUDH Research Fund.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

High-translucency 4 mol% yttria-partially stabilized zirconia (4Y-PSZ) is widely used for esthetic restorations, but sintering conditions that balance translucency and microstructural control remain unclear. This study evaluated the independent effects of peak temperature, holding time, and heating rate on the microstructure and total luminous transmittance of monolithic 4Y-PSZ. Disks were sintered at peak temperatures of 1470–1560 °C, holding times of 30–180 min, and heating rates of 3–10 °C/min. Grain size and internal defect density (≥0.5 µm) were quantified by scanning electron microscopy, and total luminous transmittance at 0.5 mm thickness was measured using a spectrophotometer. Higher peak temperatures and longer holding times increased grain size (0.481 ± 0.020 to 0.785 ± 0.035 µm, and 0.503 ± 0.037 to 0.730 ± 0.041 µm, respectively) and reduced defect density, whereas heating rate had no significant effect on either. Transmittance remained within a narrow range (approximately 40–43% at 0.5 mm) across all schedules, with 1560 °C yielding the lowest value. These findings indicate that the microstructure of monolithic 4Y-PSZ is governed primarily by peak temperature and holding time, while transmittance is relatively insensitive to the sintering schedule. Practically, a peak temperature of 1500–1530 °C with a 1–2 h hold provides a robust processing window balancing densification, grain coarsening, and optical performance for clinical workflows.

Schlagwörter

Stichwörter der Autor:innen

4Y-PSZdental materialselectron microscopyoptical transmittancesinteringspectrophotometryzirconium oxide

Autor:innen und Institutionen

  • Department of Prosthodontics and Dental Research Institute, School of Dentistry, Seoul National University, Seoul 03085, Republic of Korea.
  • Dental Life Science Research Institute, Seoul National University Dental Hospital, Seoul 03080, Republic of Korea.

ORCID-Profile: Taek-Jun Chung, Myung-Joo Kim, Bongju Kim, Young-Jun Lim

Förderung

  • Seoul National University Dental Hospital
  • SNUDH Research Fund

Zitieren

APA

Chung, T. J., Kim, M. J., Kwon, H. B., Kim, B., & Lim, Y. J. (2026). Effects of Sintering Parameters on the Microstructure and Optical Transmittance of Monolithic 4 mol% Yttria-Partially Stabilized Zirconia. Bioengineering, 13(6), 702. https://doi.org/10.3390/bioengineering13060702

Vancouver

Chung TJ, Kim MJ, Kwon HB, Kim B, Lim YJ. Effects of Sintering Parameters on the Microstructure and Optical Transmittance of Monolithic 4 mol% Yttria-Partially Stabilized Zirconia. Bioengineering. 2026;13(6):702. doi:10.3390/bioengineering13060702

BibTeX
@article{Chung2026,
  author = {Chung, Taek-Jun and Kim, Myung-Joo and Kwon, Ho-Beom and Kim, Bongju and Lim, Young-Jun},
  title = {Effects of Sintering Parameters on the Microstructure and Optical Transmittance of Monolithic 4 mol% Yttria-Partially Stabilized Zirconia},
  journal = {Bioengineering},
  year = {2026},
  volume = {13},
  number = {6},
  pages = {702},
  doi = {10.3390/bioengineering13060702}
}
Kostenlos starten →