EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Continuous Mixing of Graphite Anode Slurry: Fast-Charge Optimization Through Binder Network Tailoring

Paul Guenther, Andreas Huth, Kristian Nikolowski, Oliver Lohrberg, Mareike Partsch, Annegret Potthoff, Alexander Michaelis

Batteries · 18.07.2026 · 12 (7) · 261

DOI: 10.3390/batteries12070261 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Batteries, online erschienen am 18.07.2026. Verfasst von Paul Guenther und 6 weiteren Autor:innen. Die Arbeit wurde bisher 1-mal zitiert (Crossref) und nennt 91 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Fast-charging lithium-ion batteries require graphite anodes with low ionic transport resistance, yet systematic links between electrode manufacturing parameters and fast-charge performance remain scarce. This study shows that twin-screw extrusion (TSE) process conditions control electrode tortuosity, the geometric complexity of ionic pathways, by reshaping the binder network architecture without altering active material integrity. A central composite experimental design combined with multi-scale diagnostics identifies pore network tortuosity as the primary transport bottleneck. The optimized mild kneading condition (K4: 60 wt% kneading zone solids, 7% kneading length, gentle screw design) reduces the 8–80% state-of-charge (SOC) charging time by 14.9% relative to the intensive baseline (B1–B3: 70 wt%, 50% kneading length), matching conventional batch mixing. Regression analysis confirms a strong correlation between tortuosity and fast-charge performance (R2=0.86), whereas the correlation with charge-transfer resistance is weaker (R2=0.59). Mechanistically, mild kneading promotes reversible, sterically stabilized carboxymethyl cellulose (CMC) networks consistent with extended “loop-tail” polymer conformations. Intensive kneading is consistent with the formation of bridging gels that fail to arrest binder migration during drying and clog surface pores. A Pore-Homogeneity Index (PHI), derived from mercury porosimetry, quantifies the resulting microstructural heterogeneity, correlates with tortuosity (R2=0.76), and characterizes pore network uniformity. The results identify local stress intensity as a primary factor influencing binder network formation and support tortuosity as an adjustable design parameter in continuous anode processing.

Zitieren

APA

Guenther, P., Huth, A., Nikolowski, K., Lohrberg, O., Partsch, M., Potthoff, A., & Michaelis, A. (2026). Continuous Mixing of Graphite Anode Slurry: Fast-Charge Optimization Through Binder Network Tailoring. Batteries, 12(7), 261. https://doi.org/10.3390/batteries12070261

Vancouver

Guenther P, Huth A, Nikolowski K, Lohrberg O, Partsch M, Potthoff A, et al. Continuous Mixing of Graphite Anode Slurry: Fast-Charge Optimization Through Binder Network Tailoring. Batteries. 2026;12(7):261. doi:10.3390/batteries12070261

BibTeX
@article{Guenther2026,
  author = {Guenther, Paul and Huth, Andreas and Nikolowski, Kristian and Lohrberg, Oliver and Partsch, Mareike and Potthoff, Annegret and Michaelis, Alexander},
  title = {Continuous Mixing of Graphite Anode Slurry: Fast-Charge Optimization Through Binder Network Tailoring},
  journal = {Batteries},
  year = {2026},
  volume = {12},
  number = {7},
  pages = {261},
  doi = {10.3390/batteries12070261}
}
Kostenlos starten →