Flexural Behavior of RC Slabs Strengthened with a Reinforced Concrete Overlay
Applied Sciences · 23.11.2026 · 16 (23) · 11600
DOI: 10.3390/app162311600 ↗Kurz gefasst
Fachartikel in der Zeitschrift Applied Sciences, online erschienen am 23.11.2026. Verfasst von Mykhailo Ivaneiko und 5 weiteren Autor:innen. Die Arbeit nennt 41 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: National Research Foundation of Ukraine.
Abstract (Originalsprache)
Increasing the cross-section with concrete is a common method of strengthening reinforced concrete slabs, the effectiveness of which is determined by the conditions of composite action between the layers. Single-span RC slabs strengthened with a cast-in-place reinforced concrete overlay were tested in flexure to evaluate the influence of the interface connection type on their structural response. Two interface configurations were investigated: a substrate without intentional surface preparation or shear connectors (NIC) and a mechanically connected interface with Ø8 mm shear keys at 400 × 200 mm spacing (WIC). The tests were carried out in bending up to failure, and strains were recorded using the digital image correlation method. The load-bearing capacity of the strengthened slabs, defined by the moment at the ultimate concrete strain Mcu, exceeded that of the control slab (CS) by 143.5% for NIC and 146.1% for WIC, whereas the maximum experimental moment Mmax exceeded that of CS by 137.3% and 203.7%, respectively, and the maximum moment of the WIC slabs was 28% higher than that of NIC (17.28 kN·m versus 13.50 kN·m). A comparative analysis was performed with calculated curves based on the deformation model in accordance with DBN V.2.6-98:2009. For the strengthened slabs, the model satisfactorily predicts the moment at which the DIC surface strain at the level of the lower reinforcement reaches the nominal yield threshold (deviation up to 5%) and the bending moment at which the ultimate concrete strain is reached (deviation up to 9.1%), but does not capture the post-limit reserve of the strengthened sections: after the ultimate concrete strain was reached, the slabs continued to carry load up to 13.50 kN·m (NIC) and 17.28 kN·m (WIC), i.e., 9.8% and 40.6% above the theoretical ultimate moment. The maximum experimental deflection of WIC is close to the theoretical ultimate deflection (+1.52%), whereas that of NIC exceeds it by 44.5%, which may be associated with interlayer slip. Since these deflections correspond to different bending moments, they characterize the ultimate deformability rather than the accuracy of the model. In the analytical model, the ultimate concrete compressive strain is attained while the strain at the level of the overlay top reinforcement remains below the yield threshold; in the tests, however, the DIC surface strains measured at this level attained the nominal yield threshold in both series, and a substantial post-limit reserve developed in the sections.
Förderung
- National Research Foundation of Ukraine
Zitieren
APA
Ivaneiko, M., Klym, A., Blikharskyy, Y., Selejdak, J., Khmil, R., & Blikharskyy, Z. (2026). Flexural Behavior of RC Slabs Strengthened with a Reinforced Concrete Overlay. Applied Sciences, 16(23), 11600. https://doi.org/10.3390/app162311600
Vancouver
Ivaneiko M, Klym A, Blikharskyy Y, Selejdak J, Khmil R, Blikharskyy Z. Flexural Behavior of RC Slabs Strengthened with a Reinforced Concrete Overlay. Applied Sciences. 2026;16(23):11600. doi:10.3390/app162311600
BibTeX
@article{Ivaneiko2026,
author = {Ivaneiko, Mykhailo and Klym, Andrii and Blikharskyy, Yaroslav and Selejdak, Jacek and Khmil, Roman and Blikharskyy, Zinoviy},
title = {Flexural Behavior of RC Slabs Strengthened with a Reinforced Concrete Overlay},
journal = {Applied Sciences},
year = {2026},
volume = {16},
number = {23},
pages = {11600},
doi = {10.3390/app162311600}
}
EUVIMED