Mechanical Degradation and Damage Evolution of Double-Flawed Sandstone Under Freeze–Thaw Cycles: Effect of Fissure Inclination
Applied Sciences · 18.11.2026 · 16 (22) · 11442
DOI: 10.3390/app162211442 ↗Kurz gefasst
Fachartikel in der Zeitschrift Applied Sciences, online erschienen am 18.11.2026. Verfasst von Haiquan Wang und 6 weiteren Autor:innen. Die Arbeit nennt 45 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: National Natural Science Foundation of China, Natural Science Basic Research Foundation of Shaanxi Province, Shaanxi Provincial Postdoctoral Science Foundation Project.
Abstract (Originalsprache)
Fissured rock masses in cold regions undergo matrix deterioration and structural weakening simultaneously, and separating the contribution of each remains difficult. Intact sandstone and parallel double-flawed sandstone with fissure inclinations of 30°, 45°, and 60° were therefore tested in uniaxial compression after 0, 10, 20, 30, and 50 freeze–thaw cycles, with digital image correlation (DIC), acoustic emission (AE), and scanning electron microscopy (SEM) linking macroscopic degradation to strain localization, crack activity, and microstructural change. Peak strength and apparent elastic modulus generally decreased with freeze–thaw cycling: after 50 cycles, the peak strength of intact specimens decreased from approximately 148 to 100 MPa, while the mean apparent elastic modulus of the 60° flawed group decreased from 13.14 to 6.49 GPa (49.36% retained). Freeze–thaw treatment altered the progressive development of surface strain localization and was associated with earlier AE activity, whereas fissure inclination influenced the spatial distribution of localized deformation and the resulting failure modes. Analysis based on the ratio of rise time to amplitude (RA) and average frequency (AF) showed a growing proportion of tensile cracking in every configuration; the 45° group shifted from 55.39% shear-dominated to 68.23% tensile-dominated. SEM images recorded progressive pore enlargement, interfacial debonding, and particle spalling. This study provides experimental evidence linking freeze–thaw-induced mechanical degradation with fissure inclination-dependent damage localization and fracture evolution in double-flawed sandstone. Freeze–thaw cycling thus sets the deterioration level of the material, while fissure inclination directs where and how failure develops.
Förderung
- National Natural Science Foundation of China
- Natural Science Basic Research Foundation of Shaanxi Province
- Shaanxi Provincial Postdoctoral Science Foundation Project
- Natural Science Foundation of Hunan Province
Zitieren
APA
Wang, H., Liu, H., Jiang, S., Wang, Z., Yang, M., Tan, L., & Xue, T. (2026). Mechanical Degradation and Damage Evolution of Double-Flawed Sandstone Under Freeze–Thaw Cycles: Effect of Fissure Inclination. Applied Sciences, 16(22), 11442. https://doi.org/10.3390/app162211442
Vancouver
Wang H, Liu H, Jiang S, Wang Z, Yang M, Tan L, et al. Mechanical Degradation and Damage Evolution of Double-Flawed Sandstone Under Freeze–Thaw Cycles: Effect of Fissure Inclination. Applied Sciences. 2026;16(22):11442. doi:10.3390/app162211442
BibTeX
@article{Wang2026,
author = {Wang, Haiquan and Liu, Haofei and Jiang, Song and Wang, Zhao and Yang, Min and Tan, Lihai and Xue, Tao},
title = {Mechanical Degradation and Damage Evolution of Double-Flawed Sandstone Under Freeze–Thaw Cycles: Effect of Fissure Inclination},
journal = {Applied Sciences},
year = {2026},
volume = {16},
number = {22},
pages = {11442},
doi = {10.3390/app162211442}
}
EUVIMED