Thermal Stability and Microstructural Evolution of Cu Joints with an Ultra-Thin Sintered Layer

Siwen Shao, Chenghao Zhang, Wei Jiang, Chun Li, Xiaoqing Si, Zongjing He, Jian Cao, Yang Liu

Applied Sciences · 22.04.2026 · 16 (9) · 4108

DOI: 10.3390/app16094108 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Applied Sciences, online erschienen am 22.04.2026. Verfasst von Siwen Shao und 7 weiteren Autor:innen. Die Arbeit nennt 32 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: National Natural Science Foundation of China, State Key Laboratory of Advanced Welding and Joining.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Low-temperature Cu sintering is used as a die-bonding strategy for the third-generation power device, and the Cu-sintered joints require long-term stability at elevated temperature. In this work, we investigate the thermal stability and microstructural evolution of the Cu interconnect joints with an ultra-thin sintered layer at the temperature of 250 °C in air. The as-prepared joint shows a dense well-bonded interface with low porosity before the thermal aging test. The average shear strength of the joints increases from 85.5 MPa to 91.3 MPa after aging up to 300 h. With further increase in aging time, the shear strength begins to decrease. However, the strength remains at a high level of 69.8 MPa even after 500 h of aging, satisfying the requirements for high-temperature stability. At short aging times, the porosity within the interface reduces slightly, and the fracture exhibits distinct ductile characteristics. When the aging time exceeds 300 h, the oxide content at the interface increases from the outer region toward the inner part, and aging cracks eventually appear at the edge of the sintered layer. Therefore, it is demonstrated that the dense and thin sintered layer limits oxygen diffusion, guaranteeing the high-temperature stability of the sintered joint.

Förderung

  • National Natural Science Foundation of China
  • State Key Laboratory of Advanced Welding and Joining

Zitieren

APA

Shao, S., Zhang, C., Jiang, W., Li, C., Si, X., He, Z., Cao, J., & Liu, Y. (2026). Thermal Stability and Microstructural Evolution of Cu Joints with an Ultra-Thin Sintered Layer. Applied Sciences, 16(9), 4108. https://doi.org/10.3390/app16094108

Vancouver

Shao S, Zhang C, Jiang W, Li C, Si X, He Z, et al. Thermal Stability and Microstructural Evolution of Cu Joints with an Ultra-Thin Sintered Layer. Applied Sciences. 2026;16(9):4108. doi:10.3390/app16094108

BibTeX
@article{Shao2026,
  author = {Shao, Siwen and Zhang, Chenghao and Jiang, Wei and Li, Chun and Si, Xiaoqing and He, Zongjing and Cao, Jian and Liu, Yang},
  title = {Thermal Stability and Microstructural Evolution of Cu Joints with an Ultra-Thin Sintered Layer},
  journal = {Applied Sciences},
  year = {2026},
  volume = {16},
  number = {9},
  pages = {4108},
  doi = {10.3390/app16094108}
}
Kostenlos starten →