Comparison of Void Swelling Behavior in Wrought and Additively Manufactured 316L Stainless Steels Irradiated with 2 MeV Protons at 360 °C

Yinyin Hong, Yongchang Li, Zhihan Hu, Ching-Heng Shiau, Cheng Sun, Lin Shao

Applied Sciences · 22.02.2026 · 16 (4) · 2119

DOI: 10.3390/app16042119 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Applied Sciences, online erschienen am 22.02.2026. Verfasst von Yinyin Hong und 5 weiteren Autor:innen. Die Arbeit wurde bisher 2-mal zitiert (Crossref) und nennt 33 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Additively manufactured (AM) and wrought 316L stainless steels were irradiated with 2 MeV protons at 360 °C. Depth-resolved void swelling was quantified using cross-sectional transmission electron microscopy, with a safe-zone analysis applied to exclude near-surface and proton-range artifacts. The AM 316L exhibits significantly lower swelling than the wrought alloy. Swelling in the AM material is characterized by larger voids but a much lower void number density, whereas the wrought alloy develops smaller voids at a substantially higher density. The two alloys also display distinct dependences on local damage: in AM 316L, void size increases with local dpa while the void density remains nearly constant, whereas in wrought 316L, the void size is approximately constant and the void density increases with local dpa. These trends indicate that AM 316L has already entered a void growth-dominated regime, while wrought 316L remains in a void-nucleation-dominated regime. The reduced swelling in the AM alloy is attributed to more effective defect-recombination sinks and/or reduced vacancy mobility associated with the AM microstructure. These findings provide important insight for the evaluation and optimization of AM 316L alloys for nuclear industry applications.

Zitieren

APA

Hong, Y., Li, Y., Hu, Z., Shiau, C., Sun, C., & Shao, L. (2026). Comparison of Void Swelling Behavior in Wrought and Additively Manufactured 316L Stainless Steels Irradiated with 2 MeV Protons at 360 °C. Applied Sciences, 16(4), 2119. https://doi.org/10.3390/app16042119

Vancouver

Hong Y, Li Y, Hu Z, Shiau C, Sun C, Shao L. Comparison of Void Swelling Behavior in Wrought and Additively Manufactured 316L Stainless Steels Irradiated with 2 MeV Protons at 360 °C. Applied Sciences. 2026;16(4):2119. doi:10.3390/app16042119

BibTeX
@article{Hong2026,
  author = {Hong, Yinyin and Li, Yongchang and Hu, Zhihan and Shiau, Ching-Heng and Sun, Cheng and Shao, Lin},
  title = {Comparison of Void Swelling Behavior in Wrought and Additively Manufactured 316L Stainless Steels Irradiated with 2 MeV Protons at 360 °C},
  journal = {Applied Sciences},
  year = {2026},
  volume = {16},
  number = {4},
  pages = {2119},
  doi = {10.3390/app16042119}
}
Kostenlos starten →