A post-weld annealing strategy was developed to control the high-cycle fatigue performance of dissimilar TC11/TC17 titanium alloy linear friction welded joints. By systematically varying the stress relief annealing temperature (590, 605, 630, and 650 °C), the microstructural evolution, residual stress, and mechanical properties were investigated. The results demonstrate that increasing the annealing temperature promotes the decomposition of metastable β phase and the precipitation of fine secondary α, which raises the α phase area fraction in the fracture zone; this effect saturates above 630 °C. Concurrently, the longitudinal tensile residual stress, which reaches 400 MPa in the as-welded state, is substantially relaxed and is essentially eliminated at 630 °C. These synergistic changes enable a monotonic increase in the fatigue limit from 453.3 MPa to 512.5 MPa as the temperature rises to 630 °C, after which the property stabilizes. Fracture toughness exhibits divergent trends among the weld zones: the KIC of the weld nugget zone and the TC17-side thermo-mechanically affected zone increases with annealing temperature, while that of the TC11-side zone decreases due to the globularization of lamellar α; all three zones stabilize at approximately 33 MPa m 1/2 and 40 MPa m 1/2 , respectively. Integrating the microstructural evolution, residual stress relief, and mechanical property improvements, the optimal stress relief annealing strategy is to apply a temperature of at least 630 °C, which ensures superior fatigue resistance and microstructural stability for TC11/TC17 linear friction welded joints.

Zitieren

APA

Shen, Z., Yang, J., & Chen, X. (2026). Fatigue performance control strategy of TC11 and TC17 linear friction welded joints via annealing treatment. Frontiers in Materials, 13. https://doi.org/10.3389/fmats.2026.1882136

Vancouver

Shen Z, Yang J, Chen X. Fatigue performance control strategy of TC11 and TC17 linear friction welded joints via annealing treatment. Frontiers in Materials. 2026;13. doi:10.3389/fmats.2026.1882136

BibTeX
@article{Shen2026,
  author = {Shen, Zishi and Yang, Jun and Chen, Xianmin},
  title = {Fatigue performance control strategy of TC11 and TC17 linear friction welded joints via annealing treatment},
  journal = {Frontiers in Materials},
  year = {2026},
  volume = {13},
  doi = {10.3389/fmats.2026.1882136}
}
Kostenlos starten →