Effect of Particle Length to the Quality Particleboard Made from Sorghum Bagasse
Journal of Sylva Indonesiana · 2018
DOI: 10.32734/jsi.v1i1.423 ↗Kurz gefasst
Fachartikel in der Zeitschrift Journal of Sylva Indonesiana, 2018. Verfasst von Apri Heri Iswanto und 3 weiteren Autor:innen. Die Arbeit wurde bisher 1-mal zitiert (Crossref).
Abstract (Originalsprache)
The objective of this research was to evaluate the effect of length size particle on physical and mechanical properties of particleboard. Sorghum bagasse was cut into 3, 5, and 7 cm length size. Furthermore, particles were dried until reached of4% moisture content. Amount of 10% urea-formaldehyde (UF) resin used for binding. Hot pressing process conducted in 130C temperature for 10 minutes and 30 kg cm -2 pressure. The results showed that thickness swelling (TS) and internal bond (IB) did not fulfill of requirement of Japanese Industrial Standard (JIS) A 5908 (2003). According to all parameters, 3 cm length size of particle was resulting in the best properties.
Zitieren
APA
Iswanto, A. H., Prabuningrum, D. S., Azhar, I., & Supriyanto, S. (2018). Effect of Particle Length to the Quality Particleboard Made from Sorghum Bagasse. Journal of Sylva Indonesiana. https://doi.org/10.32734/jsi.v1i1.423
Vancouver
Iswanto AH, Prabuningrum DS, Azhar I, Supriyanto S. Effect of Particle Length to the Quality Particleboard Made from Sorghum Bagasse. Journal of Sylva Indonesiana. 2018. doi:10.32734/jsi.v1i1.423
BibTeX
@article{Iswanto2018,
author = {Iswanto, Apri Heri and Prabuningrum, Dita Sari and Azhar, Irawati and Supriyanto, Supriyanto},
title = {Effect of Particle Length to the Quality Particleboard Made from Sorghum Bagasse},
journal = {Journal of Sylva Indonesiana},
year = {2018},
doi = {10.32734/jsi.v1i1.423}
}
EUVIMED