EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Wear Mechanisms and Service Life of PVD-Coated Collar Dies in Coin Minting

Sunchai Srirod, Phanphong Kongphan

Production Engineering Archives · 01.03.2026 · 32 (1) · 34-47

DOI: 10.30657/pea.2026.32.4 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Production Engineering Archives, online erschienen am 09.03.2026. Verfasst von Sunchai Srirod und 1 weiteren Autor:innen. Die Arbeit nennt 32 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Circulating coins remain indispensable in Thailand despite rapid digitalization, with the 5-baht denomination playing a critical role. Yet, collar dies used in its minting suffer frequent wear and premature failure, increasing production costs. This study systematically evaluated two cold-work tool steels – DIN 2379 (conventional) and Böhler K490 (powder metallurgy) – uncoated and coated with titanium nitride (TiN) or chromium nitride (CrN) via arc-PVD, under industrial high-speed minting. Testing included hardness and scratch adhesion, optical/SEM–EDS wear analysis, regression-based tool life prediction, quantitative coin quality assessment, and economic evaluation. Results demonstrated that substrate–coating synergy was decisive. TiN on DIN 2379 achieved the best overall performance, sustaining ~1.5 million coins with negligible defects, while uncoated DIN 2379 failed at ~0.67 million. CrN provided intermediate life (~0.95 million) but with lower adhesion stability. In contrast, K490 systems terminated early (~0.8–1.0 million coins) due to Cu–Ni debris accumulation, despite groove wear depths remaining below 4 μm. Regression models predicted >6 million coins for K490, but these values were invalid, highlighting the inadequacy of wear-only criteria. The novelty of this work lies in experimentally confirming, under industrial Thai minting conditions, that debris – not wear depth – governs die termination and product quality. TiN-coated DIN 2379 emerged as the most reliable and cost-effective option (~175,000 Baht per million coins), providing a framework for die management that integrates wear progression, debris effects, and economic efficiency.

Zitieren

APA

Srirod, S., & Kongphan, P. (2026). Wear Mechanisms and Service Life of PVD-Coated Collar Dies in Coin Minting. Production Engineering Archives, 32(1), 34-47. https://doi.org/10.30657/pea.2026.32.4

Vancouver

Srirod S, Kongphan P. Wear Mechanisms and Service Life of PVD-Coated Collar Dies in Coin Minting. Production Engineering Archives. 2026;32(1):34-47. doi:10.30657/pea.2026.32.4

BibTeX
@article{Srirod2026,
  author = {Srirod, Sunchai and Kongphan, Phanphong},
  title = {Wear Mechanisms and Service Life of PVD-Coated Collar Dies in Coin Minting},
  journal = {Production Engineering Archives},
  year = {2026},
  volume = {32},
  number = {1},
  pages = {34--47},
  doi = {10.30657/pea.2026.32.4}
}
Kostenlos starten →