EUVIMEDEUVIMED entdecken
Crossref

Ce:GAGG and Al 2 O 3 −Ce:GAGG phosphor ceramics for laser-driven lighting: Effects of Ga 3+ substitution

Denis Yu. Kosyanov, Anastasia A. Vornovskikh, Alexey P. Zavjalov, Zlata E. Priimak, Andrei A. Leonov, Andrei A. Obraztsov, Yanbin Wang, Ziqiu Chen, Zhenzhen Zhou, Jiang Li

Journal of Advanced Ceramics · 2026-04 · 15 (4) · 9221267

DOI: 10.26599/jac.2026.9221267 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Journal of Advanced Ceramics, 2026-04. Verfasst von Denis Yu. Kosyanov und 9 weiteren Autor:innen. Die Arbeit wurde bisher 8-mal zitiert (Crossref) und nennt 39 Literaturangaben.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Monophase Ce:Gd3Al5−xGaxO12 (Ce:GAGG) with x = 0.5–3.0 and 50 vol% Al2O3−containing composite phosphor ceramics (PCs) were prepared in a pure oxygen atmosphere. The effects of Ga3+ substitution on their phase formation, microstructure, and luminescence properties were systematically investigated. For Ce:GAGG series samples, no additional phases were identified, and the distribution of Ga between the octahedral (Al/Ga)2 (0, 0, 0) and tetrahedral (Al/Ga)3 (0.375, 0, 0.25) sites of the garnet phase was clarified. For Al2O3−Ce:GAGG composites, the exchange of Al and Ga elements between the phases of garnet Ga(Al,Ga)G and oxide (Al,Ga)2O3 was revealed, and the transformation of (Al,Ga)2O3 from the α- to κ-phase (x ≥ 2.0) with the formation of elongated grains and their partial melting (x = 3) is shown. This was also reflected in a less pronounced shift of the photoluminescence peak (PL) toward shorter wavelengths for the composite series in comparison with the monophase series: with an increase in x to 3.0, the shift in the position of the PL peak of intensity by 18 nm for Al2O3−Ce:GAGG was equivalent to that for Ce:GAGG at x = 1.5. A phosphorescence phenomenon was found at x = 2.5 and 3.0 for monophasic Ce:GAGG compositions. Under the excitation of 1 W 450 nm LDs in reflection mode, 0.4 mm-thick Al2O3−Ce:GAGG with x = 0.5–1.5 had an optimum correlated color temperature of 5400–6300 K, a luminous efficiency of 123–145 lm∙W−1, and a color rendering index (Ra = 69–64). The obtained PCs showed high application potential in solid-state laser lighting.

Zitieren

APA

Kosyanov, D. Y., Vornovskikh, A. A., Zavjalov, A. P., Priimak, Z. E., Leonov, A. A., Obraztsov, A. A., Wang, Y., Chen, Z., Zhou, Z., & Li, J. (2026). Ce:GAGG and Al 2 O 3 −Ce:GAGG phosphor ceramics for laser-driven lighting: Effects of Ga 3+ substitution. Journal of Advanced Ceramics, 15(4), 9221267. https://doi.org/10.26599/jac.2026.9221267

Vancouver

Kosyanov DY, Vornovskikh AA, Zavjalov AP, Priimak ZE, Leonov AA, Obraztsov AA, et al. Ce:GAGG and Al 2 O 3 −Ce:GAGG phosphor ceramics for laser-driven lighting: Effects of Ga 3+ substitution. Journal of Advanced Ceramics. 2026;15(4):9221267. doi:10.26599/jac.2026.9221267

BibTeX
@article{Kosyanov2026,
  author = {Kosyanov, Denis Yu. and Vornovskikh, Anastasia A. and Zavjalov, Alexey P. and Priimak, Zlata E. and Leonov, Andrei A. and Obraztsov, Andrei A. and Wang, Yanbin and Chen, Ziqiu and Zhou, Zhenzhen and Li, Jiang},
  title = {Ce:GAGG and Al 2 O 3 −Ce:GAGG phosphor ceramics for laser-driven lighting: Effects of Ga 3+ substitution},
  journal = {Journal of Advanced Ceramics},
  year = {2026},
  volume = {15},
  number = {4},
  pages = {9221267},
  doi = {10.26599/jac.2026.9221267}
}
Kostenlos starten →