A Comparative Analysis of Compressive and Flexural Strength in Concrete with Partial Cement Replacement using Waste Glass Powder

Hedayat Ullah Safi, Mohammad Mukhlis Behsoodi, Mohammad Naseer Sharifi

Indonesian Journal of Material Research · 2024

DOI: 10.26554/ijmr.20242120 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Indonesian Journal of Material Research, 2024. Verfasst von Hedayat Ullah Safi und 2 weiteren Autor:innen. Die Arbeit wurde bisher 9-mal zitiert (Crossref).

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

This experimental inquiry delves into the evaluation of compressive and flexural strengths in concrete through the utilization of waste glass powder as a partial substitute for cement. Compressive strength is a key metric, indicating the concrete’s ability to effectively support structural axial loads, while flexural strength signifies its capacity to withstand deformation under bending, specifically the maximum tensile stress it can endure without fracturing when subjected to a bending moment. Certain pozzolanic materials have demonstrated the ability to enhance the mechanical strength of concrete when used as a cement replacement, and waste glass powder is among them. To address this, the experimental investigation included the substitution of cement with glass powder at different proportions (0%, 10%, 15%, 17.5%, and 20%) in both cubic and prismatic samples. Compressive strength and flexural strength tests were made following the curing of the samples for 7, 14, and 28 days. The findings indicated that the 17.5% cement replacement level exhibited a 6.07% over-strength for compressive strength and a 6.85% over-strength for flexural strength on the 28th day. However, the 15% replacement showed superior strength compared to a 10% replacement, and the 10% replacement was stronger than a 0% cement replacement. Notably, the 20% cement replacement displayed negative over-strength percentages, specifically -2.42% in compressive strength and -1.42% in flexural strength on the 28th day. This deviation raises concerns about its suitability for use in concrete applications, signifying that a 20% replacement may not be recommended.

Zitieren

APA

Safi, H. U., Behsoodi, M. M., & Sharifi, M. N. (2024). A Comparative Analysis of Compressive and Flexural Strength in Concrete with Partial Cement Replacement using Waste Glass Powder. Indonesian Journal of Material Research. https://doi.org/10.26554/ijmr.20242120

Vancouver

Safi HU, Behsoodi MM, Sharifi MN. A Comparative Analysis of Compressive and Flexural Strength in Concrete with Partial Cement Replacement using Waste Glass Powder. Indonesian Journal of Material Research. 2024. doi:10.26554/ijmr.20242120

BibTeX
@article{Safi2024,
  author = {Safi, Hedayat Ullah and Behsoodi, Mohammad Mukhlis and Sharifi, Mohammad Naseer},
  title = {A Comparative Analysis of Compressive and Flexural Strength in Concrete with Partial Cement Replacement using Waste Glass Powder},
  journal = {Indonesian Journal of Material Research},
  year = {2024},
  doi = {10.26554/ijmr.20242120}
}
Kostenlos starten →