Assessing The Influence of Three Aluminium Oxide Particle Variants in Sand Blasting on Tensile Bond Strength Between Soft Resilient Liner and Polymethyl Methacrylate Denture Base - An In Vitro Study
International Journal of Drug Delivery Technology · 04.04.2026 · 16 (89s)
DOI: 10.25258/ijddt.16.89s.39 ↗Kurz gefasst
Fachartikel in der Zeitschrift International Journal of Drug Delivery Technology, online erschienen am 04.04.2026. Verfasst von Shivangi Khare und 5 weiteren Autor:innen.
Abstract (Originalsprache)
STATEMENT OF THE PROBLEM: Adhesion failure between silicone resilient denture lining materials and denture base resin is commonly encountered in clinical practice. PURPOSE: To investigate the bond strength and adhesion of commercially available soft denture liner to alumina-abraded polymethyl methacrylate denture base resin. METHODOLOGY: The specimens were prepared using heat-cure denture base material (ACRYTON- ‘H’ Heat cure) in the moulds in denture flasks, and divided into four groups, one being control group. 3 mm of the material was cut from the thin midsection. Bonding surfaces of specimens were sandblasted at a distance of 10 mm between the surface of the specimen and the blasting tip, with different size (50, 110, 250 µm) of aluminium oxide particles (SAFE PLUS BLASTER SAND) at 2 bar for 10 seconds. Specimens were secured in the gypsum moulds, and the specimens and relining material (ACRYTON soft liner) was polymerized, were then stored in distilled water at 37oC for 1 week. The maximum tensile stress before failure was recorded for each specimen. Bond strength (in megapascal) was calculated using the following formula: Bond strength (N/mm2) = F/A {Where F is maximum force (N), and A is cross sectional area (mm2)}. The mean for different readings was tested using Analysis of Variance (ANOVA) for tensile strength. Tukey post hoc was applied to find significant difference within groups. RESULTS: The mean tensile bond strength was highest in Group II (50 µm aluminium oxide particles) (0.41 ± 0.09 MPa), followed by Group III (110 µm) (0.39 ± 0.07 MPa). The control group (0.35 ± 0.08 MPa) and Group IV (250 µm) (0.34 ± 0.05 MPa) demonstrated comparatively lower mean values. The 50 µm aluminium oxide group (Group II) demonstrated the highest percentage increase in tensile bond strength (+17.1%) compared to the control group CONCLUSIONS: findings suggest that moderate surface roughening (50 µm) enhances interfacial bonding, while larger particle size (250 µm) may adversely affect bonding efficiency.
Zitieren
APA
Khare, S., Chandu, G., Tomar, B. S., Dahiphale, R., Verma, S., & Sarvekar, T. (2026). Assessing The Influence of Three Aluminium Oxide Particle Variants in Sand Blasting on Tensile Bond Strength Between Soft Resilient Liner and Polymethyl Methacrylate Denture Base - An In Vitro Study. International Journal of Drug Delivery Technology, 16(89s). https://doi.org/10.25258/ijddt.16.89s.39
Vancouver
Khare S, Chandu G, Tomar BS, Dahiphale R, Verma S, Sarvekar T. Assessing The Influence of Three Aluminium Oxide Particle Variants in Sand Blasting on Tensile Bond Strength Between Soft Resilient Liner and Polymethyl Methacrylate Denture Base - An In Vitro Study. International Journal of Drug Delivery Technology. 2026;16(89s). doi:10.25258/ijddt.16.89s.39
BibTeX
@article{Khare2026,
author = {Khare, Shivangi and Chandu, G.S. and Tomar, Brajendra Singh and Dahiphale, Rutuja and Verma, Shubhanshu and Sarvekar, Tanmay},
title = {Assessing The Influence of Three Aluminium Oxide Particle Variants in Sand Blasting on Tensile Bond Strength Between Soft Resilient Liner and Polymethyl Methacrylate Denture Base - An In Vitro Study},
journal = {International Journal of Drug Delivery Technology},
year = {2026},
volume = {16},
number = {89s},
doi = {10.25258/ijddt.16.89s.39}
}
EUVIMED