Paste volume fraction and aggregate fineness as design parameters for 3D-printed self-activated cementless mortars: buildability, compressive anisotropy, and flexural response
Materials Science-Poland · 01.06.2026 · 44 (2) · 126-148
DOI: 10.2478/msp-2026-0022 ↗Kurz gefasst
Fachartikel in der Zeitschrift Materials Science-Poland, online erschienen am 16.11.2026. Verfasst von Jie Chen und 3 weiteren Autor:innen. Die Arbeit nennt 78 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY-NC-ND 4.0).
Abstract (Originalsprache)
Mix design for three-dimensional (3D)-printed mortars typically relies on the water-to-binder (w/b) and sand-to-binder (s/b) ratios, which become coupled when printability is held constant. This study examined whether the paste volume fraction ( V p ) and the aggregate fineness modulus (FM) can serve as practical design parameters for a self-activated ternary cementless mortar comprising ground granulated blast-furnace slag, co-fired fly ash, and fly ash, prepared without any external alkaline activator. Sixteen mixtures (s/b 1.00–1.75; FM 1.2 and 1.7; two binder compositions) were brought into a common printing window by a two-stage iso-workability procedure in which w/b and, where necessary, superplasticizer were adjusted as dependent variables. Stacking capacity ranged from 6 to 19 layers but was only weakly associated with mini-slump ( R 2 = 0.32) and unrelated to initial setting time ( R 2 = 0.04, p = 0.43). Only s/b was significantly associated with layer count ( R 2 = 0.36, p = 0.014), suggesting that the granular skeleton, rather than shape retention or setting kinetics, limited buildability. All mixtures exceeded 20 MPa at 56 days and reached about 70% of this strength within 7 days. V p described the 56-day axial compressive strength better than w/b and marginally better than s/b ( R 2 = 0.57, p < 0.001). Printed specimens matched mould-cast cubes in axial strength (mean ratio 0.98) but retained only 0.65 of it laterally; the anisotropy index (0.51–0.81) did not change with age and was not significantly affected by any design factor. FM was the only factor that significantly affected flexural strength ( p = 0.008), and it was not correlated with compressive strength; the flexural–compressive coefficient averaged 0.84 for the finer and 1.09 for the coarser sand. X-ray diffraction of the hardened pastes indicated consumption of the free lime and anhydrite supplied by the co-fired fly ash. Within the tested range, V p and FM acted mainly on different properties and can serve as complementary proportioning parameters, although the modest explained variance limits their predictive use.
Zitieren
APA
Chen, J., Korniejenko, K., Ho, C., & Lin, W. (2026). Paste volume fraction and aggregate fineness as design parameters for 3D-printed self-activated cementless mortars: buildability, compressive anisotropy, and flexural response. Materials Science-Poland, 44(2), 126-148. https://doi.org/10.2478/msp-2026-0022
Vancouver
Chen J, Korniejenko K, Ho C, Lin W. Paste volume fraction and aggregate fineness as design parameters for 3D-printed self-activated cementless mortars: buildability, compressive anisotropy, and flexural response. Materials Science-Poland. 2026;44(2):126-148. doi:10.2478/msp-2026-0022
BibTeX
@article{Chen2026,
author = {Chen, Jie and Korniejenko, Kinga and Ho, Chia-Ying and Lin, Wei-Ting},
title = {Paste volume fraction and aggregate fineness as design parameters for 3D-printed self-activated cementless mortars: buildability, compressive anisotropy, and flexural response},
journal = {Materials Science-Poland},
year = {2026},
volume = {44},
number = {2},
pages = {126--148},
doi = {10.2478/msp-2026-0022}
}
EUVIMED