Mechanical acceptability versus material stability in hot-plate-welded PVC-U/glass-fiber composite joints

Marek Kozielczyk, Kinga Mencel, Jakub Kowalczyk, Marta Paczkowska

Bulletin of the Polish Academy of Sciences Technical Sciences · 02.11.2026 · 74 (6) · 7058

DOI: 10.24425/bpasts.2026.7058 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Bulletin of the Polish Academy of Sciences Technical Sciences, online erschienen am 02.11.2026. Verfasst von Marek Kozielczyk und 3 weiteren Autor:innen. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

This study assesses the material integrity of hot-plate-welded unplasticized PVC profiles reinforced with glass-fiber composite inserts, focusing on whether cycle shortening preserves the weld-zone state beyond satisfying macroscopic strength criteria. The constituent materials were characterized to define the mechanical and thermomechanical mismatch of the hybrid system. Welded corner specimens were produced under selected parameter sets and examined by ball indentation hardness testing, stereomicroscopy, differential scanning calorimetry, and Fourier-transform infrared spectroscopy in attenuated total reflectance mode. The composite contained 52.25 wt.% glass fiber and showed higher stiffness, strength, and heat deflection temperature than PVC-U, but substantially lower deformability, confirming pronounced material asymmetry in the joint region. The weld produced at 264°C for 22 s exhibited a material response comparable to the reference condition of 264°C for 30 s. Hardness, microscopy, DSC, and FTIR-ATR revealed no detectable microstructural, thermal, or chemical deterioration after reducing plasticization time from 30 s to 22 s. Conversely, although the 270°C/21 s variant remained mechanically acceptable in terms of the failure-load criterion, it showed light-brown discoloration extending from the bead into the joint interior, lower weld-zone hardness, and a broader DSC response, indicating local thermal overexposure. These results show that mechanical acceptability does not necessarily imply material stability and that cycle-time reduction should therefore be evaluated using complementary mechanical, morphological, thermal, and chemical criteria.

Zitieren

APA

Kozielczyk, M., Mencel, K., Kowalczyk, J., & Paczkowska, M. (2026). Mechanical acceptability versus material stability in hot-plate-welded PVC-U/glass-fiber composite joints. Bulletin of the Polish Academy of Sciences Technical Sciences, 74(6), 7058. https://doi.org/10.24425/bpasts.2026.7058

Vancouver

Kozielczyk M, Mencel K, Kowalczyk J, Paczkowska M. Mechanical acceptability versus material stability in hot-plate-welded PVC-U/glass-fiber composite joints. Bulletin of the Polish Academy of Sciences Technical Sciences. 2026;74(6):7058. doi:10.24425/bpasts.2026.7058

BibTeX
@article{Kozielczyk2026,
  author = {Kozielczyk, Marek and Mencel, Kinga and Kowalczyk, Jakub and Paczkowska, Marta},
  title = {Mechanical acceptability versus material stability in hot-plate-welded PVC-U/glass-fiber composite joints},
  journal = {Bulletin of the Polish Academy of Sciences Technical Sciences},
  year = {2026},
  volume = {74},
  number = {6},
  pages = {7058},
  doi = {10.24425/bpasts.2026.7058}
}