Valorization of Sodium Silicate (Na2SiO3) Solution Waste from Coal Fly Ash Processing for the Formation of Silica Precipitate Using CO2 Capture

La Tansa Pramesti Dewi, Widya Rosita, Himawan Tri Bayu Murti Petrus, Ferian Anggara, Robertus Dhimas Dhewangga Putra

Chemistry & Chemical Technology · 25.10.2026 · 20 (3) · 483-491

DOI: 10.23939/chcht20.03.483 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Chemistry & Chemical Technology, online erschienen am 29.10.2026. Verfasst von La Tansa Pramesti Dewi und 4 weiteren Autor:innen.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Liquid waste generated from the rare earth elements recovery process through the alkaline leaching of coal fly ash (CFA) should be managed to have a positive impact on the circular economy. It contains sodium silicate (Na₂SiO₃), which can be utilized for silica production via the reaction between Na₂SiO₃ and CO₂ gas. This study aimed to examine the effect of the Na₂SiO₃ concentrations and CO₂ gas flow rates on silica formation. The concentration of the Na₂SiO₃ solution was varied at 33, 25, 20, and 16 %v/v, while the CO₂ gas flow rate was varied at 2, 3, and 4 L/min. Increasing the Na₂SiO₃ concentration increased the amount of the amorphous phase. The highest amount of amorphous SiO₂ was obtained at a concentration of 16 %v/v and at a CO₂ gas flow rate of 4 L/min, with values of 88.2% and 43.8%, respectively. The highest yield of SiO₂ in the dried solid precipitate (85.9%) was achieved at a Na₂SiO₃ concentration of 33 %v/v. Then, the highest yield of SiO₂ (80.4%) was also obtained at a CO₂ gas flow rate of 3 L/min. Conversely, a lower Na₂SiO₃ solution concentration and lower CO₂ gas flow rate resulted in high-purity precipitate products. Silica in the precipitate products was observed to be more concentrated at a Na₂SiO₃ concentration of 16%.

Zitieren

APA

Dewi, L. T. P., Rosita, W., Petrus, H. T. B. M., Anggara, F., & Putra, R. D. D. (2026). Valorization of Sodium Silicate (Na2SiO3) Solution Waste from Coal Fly Ash Processing for the Formation of Silica Precipitate Using CO2 Capture. Chemistry & Chemical Technology, 20(3), 483-491. https://doi.org/10.23939/chcht20.03.483

Vancouver

Dewi LTP, Rosita W, Petrus HTBM, Anggara F, Putra RDD. Valorization of Sodium Silicate (Na2SiO3) Solution Waste from Coal Fly Ash Processing for the Formation of Silica Precipitate Using CO2 Capture. Chemistry & Chemical Technology. 2026;20(3):483-491. doi:10.23939/chcht20.03.483

BibTeX
@article{Dewi2026,
  author = {Dewi, La Tansa Pramesti and Rosita, Widya and Petrus, Himawan Tri Bayu Murti and Anggara, Ferian and Putra, Robertus Dhimas Dhewangga},
  title = {Valorization of Sodium Silicate (Na2SiO3) Solution Waste from Coal Fly Ash Processing for the Formation of Silica Precipitate Using CO2 Capture},
  journal = {Chemistry & Chemical Technology},
  year = {2026},
  volume = {20},
  number = {3},
  pages = {483--491},
  doi = {10.23939/chcht20.03.483}
}
Kostenlos starten →