Kurz gefasst

Fachartikel in der Zeitschrift Journal of Laser Applications, online erschienen am 17.11.2026. Verfasst von Hao Chen und 5 weiteren Autor:innen. Die Arbeit nennt 20 Literaturangaben. Gefördert von: The Fundamental Research Funds for the Central Universities.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

High reflectivity and high thermal conductivity present major challenges for laser cutting of aluminum alloys. In this study, the effect of defocus distance (negative: −2 mm, zero: 0 mm, positive: +2 mm) on surface morphology, cross-sectional features, elemental distribution of Cu-rich intermetallic constituents, and microhardness of fiber laser-cut 2024-T3 aluminum alloy is investigated under fixed parameters (laser power 2.5 kW, cutting speed 5 m/min, assist gas pressure 1.3 MPa). The kerf surface exhibits horizontal, vertical, and inclined striations. Zero defocus generates the deepest surface pits and the widest kerf at the sheet mid-thickness, while negative defocus produces the longest vertical striations and the highest fraction of regular striations (87.86%). Negative defocus also yields the thinnest recast layer and the smallest inclination angle of coarse grains (16°) within the recast layer. In situ observation of melt ejection behavior shows that the ejection angle rises with increasing defocus distance, and viscous slag forms under zero and positive defocus conditions. Microstructural observation identifies crack-like features propagating along coarse grain boundaries under all defocus conditions; within fine-grain regions, these features extend perpendicular to the kerf surface. Locally measured Cu content varies near the laser-cut affected zone, decreasing from ∼28.8 wt. % in columnar grain zones to ∼23.8 wt. % in fine-grain zones. Reduced microhardness is observed in the bottom region for all tested defocus conditions, with a smaller magnitude under negative defocus.

Förderung

  • The Fundamental Research Funds for the Central Universities

Zitieren

APA

Chen, H., Zhu, Z., Yin, Q., Tian, J., Dong, Z., & Yang, S. (2026). Effect of defocus distance on surface morphology, microstructure, and Cu-rich element distribution of laser-cut 2024-T3 aluminum alloy. Journal of Laser Applications, 38(4). https://doi.org/10.2351/7.0002239

Vancouver

Chen H, Zhu Z, Yin Q, Tian J, Dong Z, Yang S. Effect of defocus distance on surface morphology, microstructure, and Cu-rich element distribution of laser-cut 2024-T3 aluminum alloy. Journal of Laser Applications. 2026;38(4). doi:10.2351/7.0002239

BibTeX
@article{Chen2026,
  author = {Chen, Hao and Zhu, Zhengqiang and Yin, Qi’an and Tian, Jiazhuang and Dong, Zihui and Yang, Shanglu},
  title = {Effect of defocus distance on surface morphology, microstructure, and Cu-rich element distribution of laser-cut 2024-T3 aluminum alloy},
  journal = {Journal of Laser Applications},
  year = {2026},
  volume = {38},
  number = {4},
  doi = {10.2351/7.0002239}
}
Kostenlos starten →