Effect of static and dynamic laser beam shaping on Fe-Al intermetallic formation in Al-Si coated 22MNB5 steel

Mir-Hamza Khan, Tahir Irfan Khan, Sharhid Jabar, Jeff Markus, Travis Stahler, Pasquale Franciosa

Journal of Laser Applications · 01.11.2026 · 38 (4)

DOI: 10.2351/7.0002206 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Journal of Laser Applications, online erschienen am 06.11.2026. Verfasst von Mir-Hamza Khan und 5 weiteren Autor:innen. Die Arbeit nennt 13 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: WMG High Value Manufacturing Catapult Centre, European Union Lasers4Maas.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Laser beam welding of Al-Si coated 22MnB5 steel is challenging due to Al enrichment from the Al-Si coating, which promotes α-ferrite and Fe(Al,Si) intermetallic (IMC) formation, degrading joint performance. This study examines the effect of static-in-source fiber and dynamic beam shaping using a coherent beam combining (CBC) laser system during overlap welding, comparing static core-only, static core-to-ring, and forward-triangle dynamic beam shaping, and correlating with microstructure, and mechanical performance. The core-only beam produced a highly concentrated heat source with limited melt-pool mixing, leading to Al accumulation (∼2.7 wt. %), a high Fe(Al,Si) area fraction (∼45%), and reduced linear joint strength of 211 ± 39 N/mm. The static core-to-ring beam did not significantly reduce Al enrichment or IMC formation due to the absence of temporal modulation. In contrast, the selected forward-triangle beam shape reduced Al content to ∼1.3 wt. % and reduced Fe(Al,Si) formation by ∼78%. This was accompanied by martensitic refinement, increased low-angle grain boundary fraction, and improved hardness distribution. The forward-triangle beam shape achieved the highest linear joint strength (472 ± 26 N/mm) and weld efficiency (58%). Overall, the selected forward-triangle beam shape effectively modified melt-pool chemistry and solidification behavior in overlap welds. Joint performance was governed by the combined effects of mitigating Fe-Al phase formation and martensitic microstructural refinement associated with the selected forward-triangle beam shape.

Förderung

  • WMG High Value Manufacturing Catapult Centre
  • European Union Lasers4Maas

Zitieren

APA

Khan, M., Khan, T. I., Jabar, S., Markus, J., Stahler, T., & Franciosa, P. (2026). Effect of static and dynamic laser beam shaping on Fe-Al intermetallic formation in Al-Si coated 22MNB5 steel. Journal of Laser Applications, 38(4). https://doi.org/10.2351/7.0002206

Vancouver

Khan M, Khan TI, Jabar S, Markus J, Stahler T, Franciosa P. Effect of static and dynamic laser beam shaping on Fe-Al intermetallic formation in Al-Si coated 22MNB5 steel. Journal of Laser Applications. 2026;38(4). doi:10.2351/7.0002206

BibTeX
@article{Khan2026,
  author = {Khan, Mir-Hamza and Khan, Tahir Irfan and Jabar, Sharhid and Markus, Jeff and Stahler, Travis and Franciosa, Pasquale},
  title = {Effect of static and dynamic laser beam shaping on Fe-Al intermetallic formation in Al-Si coated 22MNB5 steel},
  journal = {Journal of Laser Applications},
  year = {2026},
  volume = {38},
  number = {4},
  doi = {10.2351/7.0002206}
}
Kostenlos starten →