Kurz gefasst

Fachartikel in der Zeitschrift Operative Dentistry, 2024. Verfasst von W T Koh und 3 weiteren Autor:innen. Beteiligte Einrichtung: Wen Thong Koh, BDS, Faculty of Dentistry, University Malaya, Kuala Lumpur, Malaysia. Hauptthemen laut MEDLINE: Glass Ionomer Cements, Silver Compounds, Quaternary Ammonium Compounds, Shear Strength. Die Arbeit wurde bisher 1-mal zitiert (Crossref) und nennt 51 Literaturangaben.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Objectives

This study investigated the effect of different surface treatments on the shear bond strength (SBS) and failure modes of self-cured (SC) and light-cured (LC) high-viscosity glass ionomer cements (HVGICs) to silver diamine fluoride (SDF)-treated simulated carious dentin (SCD). Methods and Materials: Extracted human premolars were sectioned and pH cycled for 10 days to simulate carious dentin. The demineralized specimens were treated with 38% SDF (Riva Star) for 2 minutes, washed, stored in deionized distilled water at 37°C for 2 weeks, and subjected to the following surface treatments (n=14): T1 – no treatment (control); T2 – 10 seconds polyacrylic acid (PAA); T3 – 5 seconds phosphoric acid (PPA); T4 – 5 seconds PPA plus universal adhesive (Zipbond); and T5 – 5 seconds PPA plus resin-modified GIC adhesive (Riva bond LC). SC (Riva Self-cure HV) and LC (Riva Light-cure HV) HVGICs were applied to the conditioned specimens and stored in artificial saliva at 37°C for 1 week. SBS and failure modes were subsequently determined. Statistical analyses were performed using Kruskal-Wallis/post-hoc Mann-Whitney U and Chi-square tests (α=0.05).

Results

The highest SBS was observed when SC and LC were restored with T2 and T5, respectively. Significant differences in SBS were as follows: SC – T2, T1 > T5, T3; LC – T5, T4, T3 > T2. SC generally exhibited adhesive failures, while LC presented both adhesive and mixed failures.

Conclusion

The preferred method for preparing SDF-treated carious dentin before restoration application is PAA for SC and PPA plus RMGIC adhesive for LC HVGICs.

Schlagwörter

MeSH-Schlagwörter (MEDLINE)

Glass Ionomer CementsSilver CompoundsQuaternary Ammonium CompoundsShear StrengthDental CariesFluorides, TopicalDental BondingDentinDental Stress AnalysisHumansSurface PropertiesMaterials TestingIn Vitro TechniquesDentin-Bonding Agents

Substanzen

Glass Ionomer Cementssilver diamine fluorideSilver CompoundsQuaternary Ammonium CompoundsFluorides, TopicalDentin-Bonding Agents

Autor:innen und Institutionen

  • Wen Thong Koh, BDS, Faculty of Dentistry, University Malaya, Kuala Lumpur, Malaysia.
  • *Oon Take Yeoh, BDS, DCD, Prosthodontics MRACDS, Department of Restorative Dentistry, Faculty of Dentistry, University Malaya, Kuala Lumpur, Malaysia.
  • Noor Azlin Yahya, MDentSci, BDS, DipTrans, associate professor, Department of Restorative Dentistry, Faculty of Dentistry, University Malaya, Kuala Lumpur, Malaysia.
  • Adrian Ujin Yap, PhD, MSc, BDS, Grad Dip Psychotherapy, adjunct professor, Faculty of Dentistry, University Malaya, Kuala Lumpur, Malaysia; senior consultant, Division of Dentistry, and director of research, Ng Teng Fon…

Zitieren

APA

Koh, W. T., Yeoh, O. T., Yahya, N. A., & Yap, A. U. (2024). Effect of Surface Treatments on Shear-bond Strength of Glass Ionomer Cements to Silver Diamine Fluoride-treated Simulated Carious Dentin. Operative Dentistry. https://doi.org/10.2341/23-161-l

Vancouver

Koh WT, Yeoh OT, Yahya NA, Yap AU. Effect of Surface Treatments on Shear-bond Strength of Glass Ionomer Cements to Silver Diamine Fluoride-treated Simulated Carious Dentin. Operative Dentistry. 2024. doi:10.2341/23-161-l

BibTeX
@article{Koh2024,
  author = {Koh, W T and Yeoh, O T and Yahya, N A and Yap, A U},
  title = {Effect of Surface Treatments on Shear-bond Strength of Glass Ionomer Cements to Silver Diamine Fluoride-treated Simulated Carious Dentin},
  journal = {Operative Dentistry},
  year = {2024},
  doi = {10.2341/23-161-l}
}