Effectiveness of resin-modified glass ionomer vs composite bonding agents for orthodontic bonding: a single-center randomized controlled trial

Emil Östlund, Rage Abdullahi Ossoble, Damir Malmvind, Andrea Merzo, Ronny Rukiqi, Muteb Algharbi, Anders Magnuson, Farhan Bazargani

The Angle Orthodontist · 15.06.2026

DOI: 10.2319/112025-967.1 ↗

Kurz gefasst

Randomisierte kontrollierte Studie in der Zeitschrift The Angle Orthodontist, erschienen am 15.06.2026. Verfasst von Emil Östlund und 7 weiteren Autor:innen.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Objectives

To compare the incidence of bond failures and white spot lesions (WSLs) between brackets bonded with either light-cured resin-modified glass ionomer cement (GC Fuji Ortho LC) or light-cured composite resin (3M Transbond Plus Color Change Adhesive) after 18 months of treatment. Materials and Methods 90 patients were allocated to the trial, and 84, with a mean age of 16.7 ± 2.6 years, were analyzed. The cross-mouth method was employed in each patient, in which two diagonal quadrants (e.g., upper right and lower left, or vice versa) were randomly assigned to the FujiOrtho group, and the opposite diagonal quadrants to the Transbond group. All patients were monitored for an average of 18 months for bond failure and WSL incidence. Multilevel mixed Poisson regression with robust standard errors was used to compare the groups.

Results

Overall, failure rates were 12.9% in the FujiOrtho group and 2.1% in the Transbond group, with an adjusted relative risk (aRR) of 6.21 (95% CI: 3.89–9.94), adjusted for age, sex, maxilla/mandible, tooth position, and treating orthodontist. Overall, WSL incidence was 8.3% in the FujiOrtho group and 8.8% in the Transbond group, with an aRR of 0.95 (95% CI: 0.80–1.13).

Conclusions

Transbond Plus demonstrated a significantly lower bond failure rate compared to GC FujiOrtho LC, with a 3.6 times reduced risk of bracket failure. There were neither statistically nor clinically significant differences in the incidence of WSLs between the two groups.

Schlagwörter

Stichwörter der Autor:innen

Bond failureFixed orthodontic applianceWhite spot lesions

Zitieren

APA

Östlund, E., Ossoble, R. A., Malmvind, D., Merzo, A., Rukiqi, R., Algharbi, M., Magnuson, A., & Bazargani, F. (2026). Effectiveness of resin-modified glass ionomer vs composite bonding agents for orthodontic bonding: a single-center randomized controlled trial. The Angle Orthodontist. https://doi.org/10.2319/112025-967.1

Vancouver

Östlund E, Ossoble RA, Malmvind D, Merzo A, Rukiqi R, Algharbi M, et al. Effectiveness of resin-modified glass ionomer vs composite bonding agents for orthodontic bonding: a single-center randomized controlled trial. The Angle Orthodontist. 2026. doi:10.2319/112025-967.1

BibTeX
@article{stlund2026,
  author = {Östlund, Emil and Ossoble, Rage Abdullahi and Malmvind, Damir and Merzo, Andrea and Rukiqi, Ronny and Algharbi, Muteb and Magnuson, Anders and Bazargani, Farhan},
  title = {Effectiveness of resin-modified glass ionomer vs composite bonding agents for orthodontic bonding: a single-center randomized controlled trial},
  journal = {The Angle Orthodontist},
  year = {2026},
  doi = {10.2319/112025-967.1}
}
Kostenlos starten →