EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Influence of grinding, pressing and sintering of the powder 50.0 wt% Fe, 47.0 wt% BaTiO3 and 3.0 wt% TiO2 on morphology, microstructure, magnetic and electric properties

Milentije Lukovic, Milica Spasojevic-Savkovic, Olivera Kosic, Tanja Barudzija, Vesna Lojpur, Aleksa Maricic, Miroslav Spasojevic

Science of Sintering · 2025 · 57 (3) · 457-467

DOI: 10.2298/sos230915067l ↗

Kurz gefasst

Fachartikel in der Zeitschrift Science of Sintering, 2025. Verfasst von Milentije Lukovic und 6 weiteren Autor:innen. Die Arbeit wurde bisher 1-mal zitiert (Crossref) und nennt 63 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Ministry of Education, Science and Technological Development of the Republic of Serbia.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

A mixture of 50.0 wt% Fe, 47.0 wt% BaTiO3, and 3.0 wt% TiO2 powders is milled and then pressed and sintered. Samples sintered from ground powders have a structure consisting of plates. They consist of the crystalline phase BaFe12O19 and crystalline and amorphous phases Fe, BaTiO3, and TiO2. Samples sintered from powders ground for more than 180 min are compact and composed of BaFe12O19 crystals embedded in an amorphous matrix consisting of amorphous BaTiO3 and TiO2 phases. Magnetization of a sample ground for 220 min gradually decreases with increasing temperature up to 440?C. This decrease results from the transition of ordered domains into chaotically directed domains. Above 440?C, the thermal energy is sufficiently large to destroy ordered paramagnetic ferromagnetic and weakly ferromagnetic domains. During sample cooling in the absence of an external magnetic field, the temperature dependence of magnetization is the same as that obtained during heating in the magnetic field. However, during the sample cooling in the magnetic field, substantially higher values of magnetization are obtained. Considerably higher magnetization of the cooled sample remains even after switching off the external magnetic field. The sintered sample, previously pressed in the magnetic field, has a higher dielectric constant than the sample pressed in the absence of the magnetic field. The dielectric constant decreases with increasing frequency.

Förderung

  • Ministry of Education, Science and Technological Development of the Republic of Serbia

Zitieren

APA

Lukovic, M., Spasojevic-Savkovic, M., Kosic, O., Barudzija, T., Lojpur, V., Maricic, A., & Spasojevic, M. (2025). Influence of grinding, pressing and sintering of the powder 50.0 wt% Fe, 47.0 wt% BaTiO3 and 3.0 wt% TiO2 on morphology, microstructure, magnetic and electric properties. Science of Sintering, 57(3), 457-467. https://doi.org/10.2298/sos230915067l

Vancouver

Lukovic M, Spasojevic-Savkovic M, Kosic O, Barudzija T, Lojpur V, Maricic A, et al. Influence of grinding, pressing and sintering of the powder 50.0 wt% Fe, 47.0 wt% BaTiO3 and 3.0 wt% TiO2 on morphology, microstructure, magnetic and electric properties. Science of Sintering. 2025;57(3):457-467. doi:10.2298/sos230915067l

BibTeX
@article{Lukovic2025,
  author = {Lukovic, Milentije and Spasojevic-Savkovic, Milica and Kosic, Olivera and Barudzija, Tanja and Lojpur, Vesna and Maricic, Aleksa and Spasojevic, Miroslav},
  title = {Influence of grinding, pressing and sintering of the powder 50.0 wt% Fe, 47.0 wt% BaTiO3 and 3.0 wt% TiO2 on morphology, microstructure, magnetic and electric properties},
  journal = {Science of Sintering},
  year = {2025},
  volume = {57},
  number = {3},
  pages = {457--467},
  doi = {10.2298/sos230915067l}
}
Kostenlos starten →