EUVIMEDEUVIMED entdecken
Crossref

Effects of high-translucent zirconia thickness and resin luting agent type on shear bond strength of zirconia restorations

Keisuke Hoshino, Kei Kubochi, Hiroki Takata, Satomi Arai, Soichi Ikegami, Futoshi Komine

Journal of Prosthodontic Research · 2026

DOI: 10.2186/jpr.jpr_d_26_00136 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Journal of Prosthodontic Research, 2026. Verfasst von Keisuke Hoshino und 5 weiteren Autor:innen. Beteiligte Einrichtung: Department of Fixed Prosthodontics, Nihon University School of Dentistry, Tokyo, Japan. Die Arbeit nennt 27 Literaturangaben.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

PURPOSE: This study evaluated the effects of high-translucent zirconia thickness and resin luting agent type on shear bond strength (SBS). METHODS: In total, 352 high-translucent zirconia disks (diameter: 11.0 mm) with thicknesses of 1.0, 1.5, 2.0, and 2.5 mm were fabricated and bonded to 352 zirconia disks (diameter: 8.0 mm) using four resin luting conditions: dual polymerizing resin luting agent with 40 s of light-activated polymerization (UI40), direct composite resin with 40 s of light-activated polymerization (CM40), dual polymerizing resin luting agent without light-activated polymerization (UI0), and autopolymerizing resin luting agent (OP). Specimens were tested after 24 h in distilled water (TC0) or after 5,000 thermocycles (TC5,000). SBS, failure modes, and Knoop hardness were evaluated. RESULTS: At TC0, no significant differences in SBS were observed between the zirconia thicknesses in the UI40, CM40, and UI0 groups. At TC5,000, no significant differences were observed between the 1.0-, 1.5-, and 2.0-mm zirconia specimens in the UI40, CM40, and OP groups. UI40 and CM40 showed significantly higher SBS values than UI0 in the 1.0-, 1.5-, and 2.0-mm groups after TC5,000. However, OP did not differ significantly from UI40 and CM40 in the 2.0-mm group after TC5,000. Knoop hardness in the UI40 and CM40 groups was significantly lower in the 2.5-mm group than those at lower thicknesses. CONCLUSIONS: Bonding performance was maintained when the thickness of high-translucent zirconia was ≤2.0 mm under standardized zirconia-to-zirconia bonding conditions. The effect of the type of resin luting agent varied depending on the zirconia thickness and polymerization conditions.

Schlagwörter

Stichwörter der Autor:innen

Bond strengthHigh-translucent zirconiaKnoop hardnessResin luting agentZirconia thickness

Autor:innen und Institutionen

  • Department of Fixed Prosthodontics, Nihon University School of Dentistry, Tokyo, Japan.

Zitieren

APA

Hoshino, K., Kubochi, K., Takata, H., Arai, S., Ikegami, S., & Komine, F. (2026). Effects of high-translucent zirconia thickness and resin luting agent type on shear bond strength of zirconia restorations. Journal of Prosthodontic Research. https://doi.org/10.2186/jpr.jpr_d_26_00136

Vancouver

Hoshino K, Kubochi K, Takata H, Arai S, Ikegami S, Komine F. Effects of high-translucent zirconia thickness and resin luting agent type on shear bond strength of zirconia restorations. Journal of Prosthodontic Research. 2026. doi:10.2186/jpr.jpr_d_26_00136

BibTeX
@article{Hoshino2026,
  author = {Hoshino, Keisuke and Kubochi, Kei and Takata, Hiroki and Arai, Satomi and Ikegami, Soichi and Komine, Futoshi},
  title = {Effects of high-translucent zirconia thickness and resin luting agent type on shear bond strength of zirconia restorations},
  journal = {Journal of Prosthodontic Research},
  year = {2026},
  doi = {10.2186/jpr.jpr_d_26_00136}
}
Kostenlos starten →