SSNMR confirms silicate ion substitution in the apatitic structure of 0.8wt% Si hydroxyapatite

Marc-Krystelle Mafina, Rory M. Wilson, Gregory J. Rees, Peter Gierth, Alice C. Sullivan, Karin A. Hing

Academia Materials Science · 2023

DOI: 10.20935/acadmatsci6121 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Academia Materials Science, 2023. Verfasst von Marc-Krystelle Mafina und 5 weiteren Autor:innen. Die Arbeit nennt 49 Literaturangaben.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

This study investigates the structural location of silicon present in ‘silicate-substituted’ apatite. It has been hypothesized that silicon is present in the form of silicate groups site-specifically substituted in the hydroxyapatite lattice for phosphate groups, or that there may be an amorphous silicon-rich phase in the vicinity of the grain boundaries. Solid-state nuclear magnetic resonance (SSNMR) spectroscopy was carried out to view the elemental interactions using phosphorus (31P) and silicon (29Si) probes to confirm or refute the presence of silicate groups in relation to phosphate groups in the bulk material structure. The analysis was performed on stoichiometric hydroxyapatite (HA) and silicate-substituted hydroxyapatite (SA) with a nominal silicon content of 0.8wt%, in as-precipitated, calcined (700°C), and sintered (1,250 and 1,300°C, respectively) powder forms. XRD confirmed all forms of powder were phase pure. FTIR confirmed both hydroxyl and phosphate group functionalities in all forms of HA and SA, while silicate group functionality was only observed in all forms of SA. SSNMR using 31P- and 29Si-coupled probes demonstrated that as the crystallinity of the powders increased from the precipitate to the sintered form, the signal associated with the presence of a silicate group in the phosphate environment developed as the crystal structure became more ordered. These results support the hypothesis that in SA containing 0.8wt% silicon, silicate groups are site-specifically substituted in the hydroxyapatite lattice for phosphate groups. This observation may be key to understanding the mechanisms by which the introduction of 0.8wt% silicon enhances bone regeneration in apatitic bone graft substitute materials.

Zitieren

APA

Mafina, M., Wilson, R. M., Rees, G. J., Gierth, P., Sullivan, A. C., & Hing, K. A. (2023). SSNMR confirms silicate ion substitution in the apatitic structure of 0.8wt% Si hydroxyapatite. Academia Materials Science. https://doi.org/10.20935/acadmatsci6121

Vancouver

Mafina M, Wilson RM, Rees GJ, Gierth P, Sullivan AC, Hing KA. SSNMR confirms silicate ion substitution in the apatitic structure of 0.8wt% Si hydroxyapatite. Academia Materials Science. 2023. doi:10.20935/acadmatsci6121

BibTeX
@article{Mafina2023,
  author = {Mafina, Marc-Krystelle and Wilson, Rory M. and Rees, Gregory J. and Gierth, Peter and Sullivan, Alice C. and Hing, Karin A.},
  title = {SSNMR confirms silicate ion substitution in the apatitic structure of 0.8wt% Si hydroxyapatite},
  journal = {Academia Materials Science},
  year = {2023},
  doi = {10.20935/acadmatsci6121}
}
Kostenlos starten →