Investigation of the High Temperature Resistance of Foam Concrete Produced with Dıfferent Cem-II Type Cements

Selçuk Memiş, Hasbi Yaprak, Emre Kıvanç

Bitlis Eren Üniversitesi Fen Bilimleri Dergisi · 24.03.2026 · 15 (1) · 350-359

DOI: 10.17798/bitlisfen.1810438 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Bitlis Eren Üniversitesi Fen Bilimleri Dergisi, online erschienen am 24.03.2026. Verfasst von Selçuk Memiş und 2 weiteren Autor:innen. Die Arbeit nennt 28 Literaturangaben.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

In this study, three foam concrete mixtures—each utilizing pumice aggregate and fixed foam/water content (240–50–220 g/dm³) but differing in binder type (PKB-I: CEM II/A-M (S–L); PKB-2: CEM II/A-S; PKB-3: CEM II/A-LL)—were comprehensively examined in terms of their fresh and hardened properties, permeability indicators, and high-temperature behavior. The mixtures were produced with constant mix ratios, and parameters such as density (fresh/hardened), total water absorption, open porosity, ultrasonic pulse velocity (UPV), and compressive strength at 3, 7, and 28 days were determined. For high-temperature evaluation, the specimens were exposed to 200, 400, 600, and 800 °C, and the corresponding mass loss and strength variation (%) were calculated. The results indicated that early-age mechanical development was strongly influenced by binder chemistry, with strength ranking at day 3 following the order PKB-2 > PKB-3 > PKB-I; by day 7, these differences had narrowed, and by day 28, all three systems converged to approximately 10.5–10.8 MPa. Although PKB-2 exhibited the highest unit weight, it also demonstrated the greatest porosity and water absorption. Ultrasonic pulse velocity showed a positive correlation with density and a negative correlation with porosity within the same density range. As temperature increased, mass loss gradually rose, converging at around 18–20% at 800 °C. Limited strength gains were observed between 200 °C and 400 °C due to internal water redistribution and gel relaxation, while all mixtures exhibited significant strength reductions at ≥600 °C; the limestone-based system (PKB-3) showed more pronounced losses associated with CaCO₃ decomposition. Overall, CEM II/A-LL proved suitable for lightweight elements requiring low water absorption, CEM II/A-S for applications prioritizing early-age strength, and CEM II/A-M (S–L) provided a balanced design window between mechanical, transport, and thermal stability.

Zitieren

APA

Memiş, S., Yaprak, H., & Kıvanç, E. (2026). Investigation of the High Temperature Resistance of Foam Concrete Produced with Dıfferent Cem-II Type Cements. Bitlis Eren Üniversitesi Fen Bilimleri Dergisi, 15(1), 350-359. https://doi.org/10.17798/bitlisfen.1810438

Vancouver

Memiş S, Yaprak H, Kıvanç E. Investigation of the High Temperature Resistance of Foam Concrete Produced with Dıfferent Cem-II Type Cements. Bitlis Eren Üniversitesi Fen Bilimleri Dergisi. 2026;15(1):350-359. doi:10.17798/bitlisfen.1810438

BibTeX
@article{Memi2026,
  author = {Memiş, Selçuk and Yaprak, Hasbi and Kıvanç, Emre},
  title = {Investigation of the High Temperature Resistance of Foam Concrete Produced with Dıfferent Cem-II Type Cements},
  journal = {Bitlis Eren Üniversitesi Fen Bilimleri Dergisi},
  year = {2026},
  volume = {15},
  number = {1},
  pages = {350--359},
  doi = {10.17798/bitlisfen.1810438}
}
Kostenlos starten →