Study of the influence of the carbon component content in the composition of reaction-sintered silicon carbide ceramics on its physical and mechanical characteristics

Mikhail A. Markov, Darya A. Dyuskina, Anton N. Belyakov, Andrey G. Chekuryaev, Alina D. Bykova, Alexander N. Nikolaev

Tekhnologii bezopasnosti zhiznedeyatelnosti · 2024

DOI: 10.17223/29491665/5/4 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Tekhnologii bezopasnosti zhiznedeyatelnosti, 2024. Verfasst von Mikhail A. Markov und 5 weiteren Autor:innen.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

The reaction sintering method makes it possible to produce non-shrinkable silicon carbide materials. Combining the methods of hot slip casting and reaction sintering opens the way to obtaining products of complex shapes based on silicon carbide. To obtain reaction-sintered silicon carbide materials, formed by cold uniaxial pressing and hot slip casting, with the best structural and physical-mechanical characteristics, it is necessary to select the amount of the carbon component in the initial mixture of powders. During the work, samples with 5, 10, 15, 20 % wt. of carbon component were synthesized. For all sintered samples, the open porosity values were less than 0.4%, which is typical for reaction-sintered materials. With an increase of the carbon component, the density of the sintered pressed samples increases to reach 15% wt. of carbon in the original workpiece, after which it decreases. The increase in the density of sintered samples occurs due to the binding of all carbon present in the workpiece with silicon. Among cast ceramics, samples with 15 %wt. and 20% wt. of carbon have the highest density after sintering. Lower density of samples with 5% wt. and 10% wt. carbon is due to the fact that during siliconization, the residual porosity is filled with a lowdensity component - silicon (density 2.33 g/cm3). The structure of the sintered materials is a frame, which consists of grains of the original silicon carbide (SiCΙ), bonded through the reaction-diffusion mechanism with a “binder filler” - secondary grains of silicon carbide (SiCΙΙ). Pressed samples are characterized by greater density and, as a result, greater bending strength compared to cast ceramics. Among the pressed samples, the sample with 15 wt.% of carbon has the best properties (density 3.11 g/cm3, bending strength 398 MPa). Among the cast samples, the highest bending strength (300 MPa) is characterized by a sample with 10 wt. % of carbon. Thus, the amount of introduced soot required to obtain ceramics with high density and strength is 15% wt. of carbon for samples molded by compression, and 10% wt. for samples produced by hot slip casting.

Zitieren

APA

Markov, M. A., Dyuskina, D. A., Belyakov, A. N., Chekuryaev, A. G., Bykova, A. D., & Nikolaev, A. N. (2024). Study of the influence of the carbon component content in the composition of reaction-sintered silicon carbide ceramics on its physical and mechanical characteristics. Tekhnologii bezopasnosti zhiznedeyatelnosti. https://doi.org/10.17223/29491665/5/4

Vancouver

Markov MA, Dyuskina DA, Belyakov AN, Chekuryaev AG, Bykova AD, Nikolaev AN. Study of the influence of the carbon component content in the composition of reaction-sintered silicon carbide ceramics on its physical and mechanical characteristics. Tekhnologii bezopasnosti zhiznedeyatelnosti. 2024. doi:10.17223/29491665/5/4

BibTeX
@article{Markov2024,
  author = {Markov, Mikhail A. and Dyuskina, Darya A. and Belyakov, Anton N. and Chekuryaev, Andrey G. and Bykova, Alina D. and Nikolaev, Alexander N.},
  title = {Study of the influence of the carbon component content in the composition of reaction-sintered silicon carbide ceramics on its physical and mechanical characteristics},
  journal = {Tekhnologii bezopasnosti zhiznedeyatelnosti},
  year = {2024},
  doi = {10.17223/29491665/5/4}
}
Kostenlos starten →