EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Justification of oxidative refining of electrical-grade copper. Part 1. Oxidation period

R. S. Slobodianiuk

Theory and Practice of Metallurgy · 30.09.2026 · (3) · 80-86

DOI: 10.15802/tpm.3.2026.09 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Theory and Practice of Metallurgy, online erschienen am 30.09.2026. Verfasst von R. S. Slobodianiuk. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Purpose

To determine the parameters for removing impurities from electrical-grade secondary copper by oxidizing them with atmospheric oxygen during melting in small-capacity electric furnaces followed by permanent mold casting. Methodology. The effect of the main impurities (Fe, Si, As, Sb, Sn, Zn) on the electrical resistivity of copper was evaluated using Matthiessen’s rule and the impurity coefficients reported by K. V. Hagen-Torn. The temperatures at which the reduction of cuprous oxide by impurity elements begins were estimated by the approximate entropy method of L. P. Vladimirov based on the Gibbs–Helmholtz equation. Experimental heats of secondary copper were carried out in a 40 kg high-frequency induction furnace with a graphite crucible under a covering flux of soda ash, borax and quartz sand, and the macrostructure of the cast samples was examined.

Findings

It was shown that impurities in molten copper are oxidized mainly by cuprous oxide rather than directly by atmospheric oxygen. According to the calculations, the reduction of Cu2O by antimony, iron, tin, arsenic, zinc and silicon becomes thermodynamically possible from 394, 682, 688, 766, 1027 and 1243 K, respectively, i.e., below the melting point of copper; however, intensive oxidation of impurities begins only upon melting, when Cu2O is formed intensively. Holding the melt with an open surface for 5 min followed by flux treatment yielded samples whose chemical composition corresponds to M1 grade copper except for oxygen (0.4%). The porosity of the metal is associated with the high content of copper oxides and the Cu–Cu2O eutectic, which makes subsequent deoxidation necessary. Originality. The sequence and temperature conditions of impurity oxidation during melting of electrical-grade secondary copper in small induction furnaces were substantiated, and the need to oxidize the melt to an oxygen content of at least 0.2% to prevent hydrogen porosity was shown. Practical value. The results make it possible to predict the electrical conductivity of remelted copper from its impurity content and to set the duration of the oxidation period (5 min for a 40 kg furnace) in the production of cast contact parts for the power sector from secondary copper.

Zitieren

APA

Slobodianiuk, R. S. (2026). Justification of oxidative refining of electrical-grade copper. Part 1. Oxidation period. Theory and Practice of Metallurgy, 80-86. https://doi.org/10.15802/tpm.3.2026.09

Vancouver

Slobodianiuk RS. Justification of oxidative refining of electrical-grade copper. Part 1. Oxidation period. Theory and Practice of Metallurgy. 2026:80-86. doi:10.15802/tpm.3.2026.09

BibTeX
@article{Slobodianiuk2026,
  author = {Slobodianiuk, R. S.},
  title = {Justification of oxidative refining of electrical-grade copper. Part 1. Oxidation period},
  journal = {Theory and Practice of Metallurgy},
  year = {2026},
  number = {3},
  pages = {80--86},
  doi = {10.15802/tpm.3.2026.09}
}
Kostenlos starten →