Influence of heating temperature and cooling rate on the formation of structural component steel during hardening
Theory and Practice of Metallurgy · 30.06.2023 · (2) · 10-15
DOI: 10.15802/tpm.2.2023.02 ↗Kurz gefasst
Fachartikel in der Zeitschrift Theory and Practice of Metallurgy, online erschienen am 30.06.2023. Verfasst von N. Yu. Filonenko und 3 weiteren Autor:innen. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).
Abstract (Originalsprache)
The formation of structural components starts with the hardening of steels. Therefore, it is important to study the influence of heating temperature and cooling rate of the melt on the formation of structural components of steels. Purpose of research is to investigate the influence of thermokinetic crystallization factors (heating temperature and cooling rate of the melt) on the formation of structural components, the liquation of elements, and the morphology of dendrites.
Methods
Microstructure test, X-ray microanalysis, X-ray diffraction analysis and surface etching of samples with nital and a hot solution of sodium picrate were used to determine the peculiarities of the structural state of steels.
Results
In the paper, a study of steel specimens of the similar chemical composition is carried out: after continuous casting and after heating above the liquidus line to 50°C, 150°C and cooling at rates of 10–104 °C/s. The morphology of iron dendrites and structural components of steels after continuous casting and after heating above the liquidus line to 50°C, 150°C and cooling at rates of 10–10 4 °C/s are compared. Scientific novelty. It is found out that heating above the liquidus line to 50°C, 150°C and cooling at rates of 10–104°C/s affects the morphology, sizes, and interdendritic space of iron dendrites. After heating to 50°C, 150°C and cooling at the rate of 10°C/s, the size of dendrites decreases to 50–60% and the interdendritic space to 30–40%, compared to the continuous casting in the central part. During heating to 50°C and at cooling rate of 103°C/s, we observe the formation of individual dendrites, which have smaller sizes and interdendritic distance compared to continuous casting at the same cooling rates. At heating temperature of 150 °C, the formation of individual dendrites, which do not have second-order axes, occurs already at cooling rate of 102°C/s. In addition, we observe a decrease in the content of manganese and silicon in the interdendritic space compared to the continuous casting at all cooling rates. This indicates more uniform distribution of manganese and silicon between the structural components. Practical relevance. The use of the results obtained will contribute to development of technologies for obtaining steels with a more uniform structure.
Zitieren
APA
Filonenko, N. Y., Babachenko, O. I., Kononenko, G. A., & Volchuk, V. M. (2023). Influence of heating temperature and cooling rate on the formation of structural component steel during hardening. Theory and Practice of Metallurgy, 10-15. https://doi.org/10.15802/tpm.2.2023.02
Vancouver
Filonenko NY, Babachenko OI, Kononenko GA, Volchuk VM. Influence of heating temperature and cooling rate on the formation of structural component steel during hardening. Theory and Practice of Metallurgy. 2023:10-15. doi:10.15802/tpm.2.2023.02
BibTeX
@article{Filonenko2023,
author = {Filonenko, N. Yu. and Babachenko, O. I. and Kononenko, G. A. and Volchuk, V. M.},
title = {Influence of heating temperature and cooling rate on the formation of structural component steel during hardening},
journal = {Theory and Practice of Metallurgy},
year = {2023},
number = {2},
pages = {10--15},
doi = {10.15802/tpm.2.2023.02}
}
EUVIMED