Fachartikel in der Zeitschrift Journal of Testing and Evaluation, online erschienen am 29.01.2026. Verfasst von Shuling Gao und 1 weiteren Autor:innen. Die Arbeit wurde bisher 1-mal zitiert (Crossref) und nennt 64 Literaturangaben. Gefördert von: National Natural Science Foundation of China, Natural Science Foundation of Hebei Province, S&T Program of Hebei.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

This study aims to address the issues of high self-weight, increased brittleness at high temperatures, and limited thermal resistance of ultra-high-performance concrete (UHPC) by introducing lightweight aggregate (LWA) to prepare lightweight ultra-high-performance concrete (L-UHPC). Using a systematic comparative approach, the residual flexural strength, toughness, crack evolution, and microstructural characteristics of UHPC and L-UHPC were investigated at 20°C, 200°C, 400°C, and 600°C. Additionally, acoustic emission technology was employed to elucidate the bending damage mechanism. The results showed that the density of L-UHPC was 1,990.4 kg/m3, significantly lower than that of UHPC (2,442.0 kg/m3). At room temperature, the flexural strength of L-UHPC reached 21.8 MPa, slightly lower than that of UHPC (23.4 MPa). At 200°C, the strength of both materials increased; however, at 600°C, the residual flexural strength of L-UHPC decreased by 17.1 %, a smaller reduction compared to UHPC. Rise time/amplitude–average frequency analysis shows that at temperatures of 400°C and above, the shear crack ratio of UHPC increases to 70.39 %, while that of L-UHPC remains relatively low (66.6 %), indicating superior ductility retention capability and reflecting the mitigating effect of lightweight aggregates on interface damage. b-value analysis further indicates that at 600°C, when the b-values of UHPC and L-UHPC are greater than 0.5 and 0.7, respectively, both materials can maintain a certain level of load-bearing capacity and overall stability. Scanning electron microscopy results validated this trend, showing that at temperatures above 200°C, both UHPC and L-UHPC exhibited cracks in the interface transition zone and fiber–matrix interface, but the damage was more severe in UHPC. In summary, the introduction of LWA effectively enhances the high-temperature resistance of UHPC, providing a theoretical basis and engineering references for the development of high-temperature-resistant lightweight concrete and postfire structural assessment.

Förderung

  • National Natural Science Foundation of China
  • Natural Science Foundation of Hebei Province
  • S&T Program of Hebei

Zitieren

APA

Gao, S., & Tian, M. (2026). Comparative Study on Flexural Damage Evolution of Ultra-high Performance Concrete and Lightweight Ultra-high Performance Concrete after High-Temperature Exposure. Journal of Testing and Evaluation, 54(3). https://doi.org/10.1520/jte20250158

Vancouver

Gao S, Tian M. Comparative Study on Flexural Damage Evolution of Ultra-high Performance Concrete and Lightweight Ultra-high Performance Concrete after High-Temperature Exposure. Journal of Testing and Evaluation. 2026;54(3). doi:10.1520/jte20250158

BibTeX
@article{Gao2026,
  author = {Gao, Shuling and Tian, Mengyuan},
  title = {Comparative Study on Flexural Damage Evolution of Ultra-high Performance Concrete and Lightweight Ultra-high Performance Concrete after High-Temperature Exposure},
  journal = {Journal of Testing and Evaluation},
  year = {2026},
  volume = {54},
  number = {3},
  doi = {10.1520/jte20250158}
}
Kostenlos starten →