Assessment of surface hardness and impact strength of denture base resins reinforced with silver–titanium dioxide and silver–zirconium dioxide nanoparticles: In vitro study

Eman Alwan Erhim, Manal A. Abbood, Halemah T. Halbos

Open Engineering · 21.10.2024 · 14 (1)

DOI: 10.1515/eng-2024-0064 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Open Engineering, online erschienen am 21.10.2024. Verfasst von Eman Alwan Erhim und 2 weiteren Autor:innen. Die Arbeit wurde bisher 5-mal zitiert (Crossref) und nennt 34 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Polymethyl methacrylate (PMMA) is frequently utilised for fabricating denture bases due to its perfect qualities. However, a significant issue with this resin is the occurrence of frequent fractures caused by heavy chewing power, resulting in early cracks and fractures during clinical use. This study investigates the influence of silver, titanium dioxide, and silver zirconia nanoparticles on the surface hardness and impact strength of self-cured denture base. The samples were categorised into four categories according to the incorporation of different nanoparticles. The samples were divided into three subgroups based on the nanoparticle content: 0.1, 0.3, and 0.5% of TiO 2 and ZrO 2 . Each group had a set ratio of 0.3% Ag as an antibacterial agent. Except for the fourth group (Group D), a combination of 0.05, 0.15, and 0.25% of TiO 2 and ZrO 2 , along with 0.3% Ag, was utilised to investigate their collective impact. The Shore D hardness and Charpy test were employed to quantify the surface hardness and impact strength, respectively. The samples were subjected to X-ray diffraction analysis and field emission-scanning electron microscopy to characterise nanoparticles and ascertain the structure of acrylic samples. All nanoparticle-modified samples showed a substantial improvement in surface hardness compared to the control group. The maximum hardness value was seen in the samples containing 0.3% Ag–0.3% TiO 2 and 0.3% Ag–0.5% ZrO 2 . The samples treated with 0.3% Ag and 0.3% TiO 2 showed the maximum impact strength. The incorporation of Ag and ZrO 2 hinders the ability to withstand impact strength. The samples treated with 0.3% Ag, 0.15% TiO 2 , and 0.15% ZrO 2 exhibited an augmentation in impact strength. Modified samples in all groups showed a colour change, which required colour modifiers.

Zitieren

APA

Erhim, E. A., Abbood, M. A., & Halbos, H. T. (2024). Assessment of surface hardness and impact strength of denture base resins reinforced with silver–titanium dioxide and silver–zirconium dioxide nanoparticles: In vitro study. Open Engineering, 14(1). https://doi.org/10.1515/eng-2024-0064

Vancouver

Erhim EA, Abbood MA, Halbos HT. Assessment of surface hardness and impact strength of denture base resins reinforced with silver–titanium dioxide and silver–zirconium dioxide nanoparticles: In vitro study. Open Engineering. 2024;14(1). doi:10.1515/eng-2024-0064

BibTeX
@article{Erhim2024,
  author = {Erhim, Eman Alwan and Abbood, Manal A. and Halbos, Halemah T.},
  title = {Assessment of surface hardness and impact strength of denture base resins reinforced with silver–titanium dioxide and silver–zirconium dioxide nanoparticles: In vitro study},
  journal = {Open Engineering},
  year = {2024},
  volume = {14},
  number = {1},
  doi = {10.1515/eng-2024-0064}
}
Kostenlos starten →