Laser-induced damage thresholds of photoresists for high-performance 3D-printed micro-optics in the visible and near-infrared
Optical Materials Express · 01.11.2026 · 16 (11) · 3946
DOI: 10.1364/ome.614365 ↗Kurz gefasst
Fachartikel in der Zeitschrift Optical Materials Express, online erschienen am 29.10.2026. Verfasst von Sebastian Klein und 4 weiteren Autor:innen. Die Arbeit wurde bisher 1-mal zitiert (Crossref) und nennt 38 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Deutsche Forschungsgemeinschaft, Bundesministerium für Forschung, Technologie und Raumfahrt, Ministerium für Wissenschaft, Forschung und Kunst Baden-Württemberg.
Abstract (Originalsprache)
Two-photon polymerization has emerged as a powerful technique for fabricating high-quality micro-optical components for applications such as endoscopy, optical trapping, compact lasers, and micromachining. For many of these uses, the laser-induced damage threshold of the employed photoresists is a key parameter. In this work, we systematically investigate the damage behavior of the commercial two-photon polymerization photoresists IP-S, IPX-S, and IPX-Clear under femtosecond pulsed irradiation at 1040 nm and 520 nm, as well as continuous-wave irradiation at 1030 nm. Damage tests are performed on printed microstructures using automated exposure and optical inspection procedures that enable a comparative assessment of the three materials. We observe clear differences in damage behavior depending on resist type, wavelength, and irradiation regime. Overall, all three photoresists exhibit broadly comparable performance under all tested exposure conditions, with IP-S yielding the highest damage threshold throughout, although in most cases only by a small margin. The damage threshold fluences are in the range of 3 mJ/cm 2 to 140 mJ/cm 2 in pulsed operation and 0.3 MW/cm 2 to 3 MW/cm 2 for continuous-wave irradiation. The results provide practical guidance for selecting two-photon polymerization photoresists for micro-optical components intended for high-power and ultrafast laser applications.
Förderung
- Deutsche Forschungsgemeinschaft
- Bundesministerium für Forschung, Technologie und Raumfahrt
- Ministerium für Wissenschaft, Forschung und Kunst Baden-Württemberg
- Carl Zeiss Foundation
- European Research Council
- European Innovation Council
- European Union
- European Commission
Zitieren
APA
Klein, S., Didychenko, D., Siegle, L., Ahmed, M. A., & Giessen, H. (2026). Laser-induced damage thresholds of photoresists for high-performance 3D-printed micro-optics in the visible and near-infrared. Optical Materials Express, 16(11), 3946. https://doi.org/10.1364/ome.614365
Vancouver
Klein S, Didychenko D, Siegle L, Ahmed MA, Giessen H. Laser-induced damage thresholds of photoresists for high-performance 3D-printed micro-optics in the visible and near-infrared. Optical Materials Express. 2026;16(11):3946. doi:10.1364/ome.614365
BibTeX
@article{Klein2026,
author = {Klein, Sebastian and Didychenko, Denys and Siegle, Leander and Ahmed, Marwan Abdou and Giessen, Harald},
title = {Laser-induced damage thresholds of photoresists for high-performance 3D-printed micro-optics in the visible and near-infrared},
journal = {Optical Materials Express},
year = {2026},
volume = {16},
number = {11},
pages = {3946},
doi = {10.1364/ome.614365}
}