Performance of MoS 2 -alloyed-TiAlSiN-coated cutting tools in dry turning of Ti-6Al-4V alloy

Job Wambua, Fredrick Mwema, Wai-Lok Woo, Guillaume Zoppi, Esther Akinlabi

Proceedings of the Institution of Mechanical Engineers, Part L: Journal of Materials: Design and Applications · 03.11.2026

DOI: 10.1177/14644207261493907 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Proceedings of the Institution of Mechanical Engineers, Part L: Journal of Materials: Design and Applications, online erschienen am 03.11.2026. Verfasst von Job Wambua und 4 weiteren Autor:innen. Die Arbeit nennt 63 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY-NC 4.0).

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Machining titanium alloys is challenged by high friction and temperature at the tool–workpiece interface, leading to rapid tool wear and poor surface integrity. While cutting fluids during machining have been used to avert this, they have been observed to induce irreversible chemical reactions with the machined surfaces, while also presenting manufacturers with additional cutting fluid purchase, use, and disposal costs, in addition to environmental and health concerns. This has motivated a shift towards dry machining. This study investigates the performance of MoS 2 -alloyed TiAlSiN thin film coatings (referred to as n :MoS 2 ) deposited by magnetron sputtering on tungsten carbide cutting tools for dry rough turning of Ti-6Al-4V alloy. After deposition, the MoS 2 -alloyed coatings maintained mechanical properties comparable to the TiAlSiN thin films (H ∼ 10 GPa and H/E ∼ 0.06), while significantly improving the tribological behaviour of the coated tools (coefficient of friction: TiAlSiN ∼ 0.16 and n :MoS 2 ∼ 0.13). Moreover, the n : MoS 2 -coated tools exhibited reduced and steady cutting temperatures, smoother chip flow, and the lowest flank wear, VB B (∼0.191 mm), corresponding to wear reductions of approximately 71% compared to the as-manufactured (VB B = 0.651 mm) and 20% relative to TiAlSiN-only coated tools (VB B = 0.239 mm). The enhanced performance was attributed to the effective self-lubrication and improved heat dissipation at the cutting interface. These results demonstrate the strong potential of MoS 2 -alloyed TiAlSiN coatings for enabling high-performance, environmentally sustainable dry machining of titanium alloys.

Zitieren

APA

Wambua, J., Mwema, F., Woo, W., Zoppi, G., & Akinlabi, E. (2026). Performance of MoS 2 -alloyed-TiAlSiN-coated cutting tools in dry turning of Ti-6Al-4V alloy. Proceedings of the Institution of Mechanical Engineers, Part L: Journal of Materials: Design and Applications. https://doi.org/10.1177/14644207261493907

Vancouver

Wambua J, Mwema F, Woo W, Zoppi G, Akinlabi E. Performance of MoS 2 -alloyed-TiAlSiN-coated cutting tools in dry turning of Ti-6Al-4V alloy. Proceedings of the Institution of Mechanical Engineers, Part L: Journal of Materials: Design and Applications. 2026. doi:10.1177/14644207261493907

BibTeX
@article{Wambua2026,
  author = {Wambua, Job and Mwema, Fredrick and Woo, Wai-Lok and Zoppi, Guillaume and Akinlabi, Esther},
  title = {Performance of MoS 2 -alloyed-TiAlSiN-coated cutting tools in dry turning of Ti-6Al-4V alloy},
  journal = {Proceedings of the Institution of Mechanical Engineers, Part L: Journal of Materials: Design and Applications},
  year = {2026},
  doi = {10.1177/14644207261493907}
}
Kostenlos starten →