Effect of final cooling temperature to microstructure and property relationship of V-N microalloyed X70 pipeline steel

Chufei Han, Haijian Xu, Hua Zhang, Bo Yang, Zhaozhen Cai, Xin Che, Lijia Chen

Ironmaking & Steelmaking: Processes, Products and Applications · 08.01.2026

DOI: 10.1177/03019233251411947 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Ironmaking & Steelmaking: Processes, Products and Applications, online erschienen am 08.01.2026. Verfasst von Chufei Han und 6 weiteren Autor:innen. Die Arbeit wurde bisher 1-mal zitiert (Crossref) und nennt 33 Literaturangaben. Gefördert von: China Postdoctoral Science Foundation funded project.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Herein, the final cooling temperatures (FCTs) are the key process parameters to achieve high strength and toughness combination in V-N microalloyed X70 pipeline steels. This research shows that the steels primarily consisted of polygonal ferrite (PF) and a small quantity of pearlite (P) phase at the FCT of 630 °C, while the PF and a small fraction of granular bainite (GB) and acicular ferrite (AF) were obtained at 580 °C. As the FCTs decrease from 580 °C to 450 °C, the proportion of AF and GB gradually increases. The AF was composed of fine non-parallel ferrite platelet structures with higher dislocations densities compared with other phases. The nanoscale precipitates were divided into two types under all the FCTs, large-scale Ti(C, N) precipitates of diameter 20–50 nm that precipitated at high temperatures and small V(C, N) precipitates of diameter 5–20 nm at low temperatures, which significantly contributed toward strength-toughness. As the FCTs decrease from 630 °C to 450 °C, the yield strength −20 °C impact energy and drop-weight tear test properties first increased to 565 ± 7 MPa, 505 ± 9 J and 99 ± 1% at 520 °C, and finally decreased to 520 ± 6 MPa, 256 ± 9 J and 82 ± 2% at 450 °C. The optimum microstructure and mechanical properties were obtained at the FCT of 520 °C. The fine-grain strengthening and precipitation strengthening played a crucial role in affecting the thermo-mechanical properties in this steel, such that fine-grain strengthening of 37.5%, and precipitation strengthening of 32.3% at the FCT of 520 °C. The transformation strengthening from AF and precipitation hardening from high fraction of 5–20 nm V(C, N) precipitates played a crucial role in improving the low-temperature toughness and strength.

Förderung

  • China Postdoctoral Science Foundation funded project

Zitieren

APA

Han, C., Xu, H., Zhang, H., Yang, B., Cai, Z., Che, X., & Chen, L. (2026). Effect of final cooling temperature to microstructure and property relationship of V-N microalloyed X70 pipeline steel. Ironmaking & Steelmaking: Processes, Products and Applications. https://doi.org/10.1177/03019233251411947

Vancouver

Han C, Xu H, Zhang H, Yang B, Cai Z, Che X, et al. Effect of final cooling temperature to microstructure and property relationship of V-N microalloyed X70 pipeline steel. Ironmaking & Steelmaking: Processes, Products and Applications. 2026. doi:10.1177/03019233251411947

BibTeX
@article{Han2026,
  author = {Han, Chufei and Xu, Haijian and Zhang, Hua and Yang, Bo and Cai, Zhaozhen and Che, Xin and Chen, Lijia},
  title = {Effect of final cooling temperature to microstructure and property relationship of V-N microalloyed X70 pipeline steel},
  journal = {Ironmaking & Steelmaking: Processes, Products and Applications},
  year = {2026},
  doi = {10.1177/03019233251411947}
}
Kostenlos starten →