Analysis of the formation of slag groove defects during the continuous casting of the round billets of 38CrMoAl steel
Ironmaking & Steelmaking: Processes, Products and Applications · 2026-11 · 53 (9) · 2014-2025
DOI: 10.1177/03019233251349884 ↗Kurz gefasst
Fachartikel in der Zeitschrift Ironmaking & Steelmaking: Processes, Products and Applications, online erschienen am 16.06.2025. Verfasst von Yuanhui Qiu und 5 weiteren Autor:innen. Die Arbeit nennt 55 Literaturangaben. Gefördert von: National Natural Science Foundation of China.
Abstract (Originalsprache)
38CrMoAl steel (Al = 0.8–1.1 wt%) is valued for its excellent physical properties but faces challenges due to its high-Al content, which can react with SiO 2 in mould slag during continuous casting, degrading slag performance. In view of the frequent occurrence of solid crusts in the slag pool and groove defects on the round billet surface, this study systematically investigated the in-service slag and elucidated the occurrence mechanism of groove defects. As the operation proceeded, the steel–slag reaction approached equilibrium: (SiO 2 ) content decreased to about 9 wt%, while (Al 2 O 3 ) increased to approximately 38 wt% after the third heat. These significant compositional shifts induced a sharp increase in viscosity, break temperature and melting temperature of the slag. Concurrently, the simpler structures Q n ( n = 0, 1, 2) gradually aggregated to form complex structures Q n ( n = 3, 4, 5), and as a result, the melting and flow properties deteriorated significantly. Consequently, solid crusts formed in the slag pool and were transported into slag channels via liquid slag infiltration. During shell withdrawal, inadequate lubrication of the slag film caused by solidified crusts would eventually cause the formation of groove defects on the billet surface along the withdrawal direction. This issue could be mitigated by adding fluxing agents to stabilise post-reaction slag performance.
Förderung
- National Natural Science Foundation of China
Zitieren
APA
Qiu, Y., Zhao, L., Chen, S., Lu, C., Wang, Q., & He, S. (2026). Analysis of the formation of slag groove defects during the continuous casting of the round billets of 38CrMoAl steel. Ironmaking & Steelmaking: Processes, Products and Applications, 53(9), 2014-2025. https://doi.org/10.1177/03019233251349884
Vancouver
Qiu Y, Zhao L, Chen S, Lu C, Wang Q, He S. Analysis of the formation of slag groove defects during the continuous casting of the round billets of 38CrMoAl steel. Ironmaking & Steelmaking: Processes, Products and Applications. 2026;53(9):2014-2025. doi:10.1177/03019233251349884
BibTeX
@article{Qiu2026,
author = {Qiu, Yuanhui and Zhao, Li and Chen, Shoujie and Lu, Chunxiao and Wang, Qiangqiang and He, Shengping},
title = {Analysis of the formation of slag groove defects during the continuous casting of the round billets of 38CrMoAl steel},
journal = {Ironmaking & Steelmaking: Processes, Products and Applications},
year = {2026},
volume = {53},
number = {9},
pages = {2014--2025},
doi = {10.1177/03019233251349884}
}
EUVIMED