Thickness-aware process-window mapping for selective SiC skin removal and re-densification during C/SiC chemical vapor infiltration

Kang Guan, Weikang Jiang, Ming Lv, Cheng Peng, Qing Zhang, Xiaohui Yang, Longteng Bai

Journal of Composite Materials · 16.11.2026

DOI: 10.1177/00219983261509428 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Journal of Composite Materials, online erschienen am 16.11.2026. Verfasst von Kang Guan und 6 weiteren Autor:innen. Die Arbeit nennt 47 Literaturangaben. Gefördert von: Basic and Applied Basic Research Foundation of Guangdong Province, National Natural Science Foundation of China.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Surface pore closure during isothermal chemical vapor infiltration (ICVI) limits precursor access to C/SiC preforms, leaving residual porosity and density nonuniformity. Selective SiC skin removal reopens gas pathways but also removes deposited matrix and requires recovery time. A material-conserving dual-porosity finite-volume model maps this trade-off. Calibrated against digitized CT density data, the model matches the density trajectory with 0.597% MAPE. A 122-case CVI-removal-CVI screen at three specimen thicknesses (5, 10 and 20 mm) provides three discrete design points rather than a continuous map. Tested schedules at 5 mm give no robust uniformity benefit: the least adverse case still widens the spread by −0.0027 g cm −3 . At 10 mm the gain is positive and grid-converged (0.0044–0.0054 g cm −3 across two independent refinement axes, ±10%) but stays below the 0.010 g cm −3 significance gate, so it is reported as a direction. At 20 mm, early partial removal at a 2 mm depth reduces density spread by 0.0269 g cm −3 on the base 40 × 20 grid and by 0.0223–0.0269 g cm −3 across both refinement axes (2.2–2.7 times the gate), at a retained-density penalty of 0.0094 g cm −3 ; an absolute-depth scan shows the gain rising monotonically with depth, so no normalized depth has special status. This 20 mm benefit is invariant across a nine-point axial-depletion and boundary-concentration set (0.02,682–0.02,691 g cm −3 ), and the schedule ranking is unchanged for rate multipliers from ×0.5 to ×1.5, though its magnitude scales with rate. The results turn SiC skin removal into a thickness-thresholded process-window rule.

Förderung

  • Basic and Applied Basic Research Foundation of Guangdong Province
  • National Natural Science Foundation of China

Zitieren

APA

Guan, K., Jiang, W., Lv, M., Peng, C., Zhang, Q., Yang, X., & Bai, L. (2026). Thickness-aware process-window mapping for selective SiC skin removal and re-densification during C/SiC chemical vapor infiltration. Journal of Composite Materials. https://doi.org/10.1177/00219983261509428

Vancouver

Guan K, Jiang W, Lv M, Peng C, Zhang Q, Yang X, et al. Thickness-aware process-window mapping for selective SiC skin removal and re-densification during C/SiC chemical vapor infiltration. Journal of Composite Materials. 2026. doi:10.1177/00219983261509428

BibTeX
@article{Guan2026,
  author = {Guan, Kang and Jiang, Weikang and Lv, Ming and Peng, Cheng and Zhang, Qing and Yang, Xiaohui and Bai, Longteng},
  title = {Thickness-aware process-window mapping for selective SiC skin removal and re-densification during C/SiC chemical vapor infiltration},
  journal = {Journal of Composite Materials},
  year = {2026},
  doi = {10.1177/00219983261509428}
}
Kostenlos starten →