Evaluation of Mode-I fracture toughness and failure mechanisms in carbon fibre/epoxy composites interleaved with a meltable copolyamide veil
Journal of Composite Materials · 2025-11 · 59 (27) · 3075-3087
DOI: 10.1177/00219983251341631 ↗Kurz gefasst
Fachartikel in der Zeitschrift Journal of Composite Materials, online erschienen am 16.05.2025. Verfasst von Michael Jurdana und 3 weiteren Autor:innen. Die Arbeit wurde bisher 6-mal zitiert (Crossref) und nennt 38 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY-NC 4.0). Gefördert von: Victorian Higher Education State Investment Fund.
Abstract (Originalsprache)
Interleaving of thermoplastic veils within carbon fibre composites is a method commonly utilised to increase the fracture toughness of composite materials. Previous studies have presented a range of fracture toughness values attributed to the inclusion of polyamide based thermoplastic veils; however, a large portion of these have remained focused on the use of veils that retain their fibre structure during the laminate cure cycle. This study sets out to explore the Mode-I fracture toughness and resultant failure mechanisms of a carbon/epoxy composite interleaved with a low-melt copolyamide thermoplastic veil at different areal densities. The results reveal that the thermoplastic veil polymer successfully precipitated from the initial veil fibre structure during the cure cycle resulting in a phase transformation from veil fibres to bead-like particles across the interlayer. As the veil density is increased, there is a decrease in the Mode-I fracture toughness with a reduction of 23%, 33% and 52% for 8, 14 and 20 g/m 2 veil configurations. Fractography of the fracture surface revealed the weak interface between the phase separated Co-PA particle and epoxy matrix as the primary failure mechanism across all interleaved laminates. Microscopic analysis demonstrated that the use of low-melt copolyamide veils resulted in a semi-uniform distribution of precipitated thermoplastic particles in low veil densities (8 g/m 2 ), however led to a slightly larger particle size and onset of agglomerations as the density was increased (14 g/m 2 ) before forming a bi-continuous phase at high veil densities (20 g/m 2 ) leading to larger reductions in the calculated fracture toughness.
Förderung
- Victorian Higher Education State Investment Fund
Zitieren
APA
Jurdana, M., Eisenbart, B., Nikzad, M., & Pietro, A. D. (2025). Evaluation of Mode-I fracture toughness and failure mechanisms in carbon fibre/epoxy composites interleaved with a meltable copolyamide veil. Journal of Composite Materials, 59(27), 3075-3087. https://doi.org/10.1177/00219983251341631
Vancouver
Jurdana M, Eisenbart B, Nikzad M, Pietro AD. Evaluation of Mode-I fracture toughness and failure mechanisms in carbon fibre/epoxy composites interleaved with a meltable copolyamide veil. Journal of Composite Materials. 2025;59(27):3075-3087. doi:10.1177/00219983251341631
BibTeX
@article{Jurdana2025,
author = {Jurdana, Michael and Eisenbart, Boris and Nikzad, Mostafa and Pietro, Adriano Di},
title = {Evaluation of Mode-I fracture toughness and failure mechanisms in carbon fibre/epoxy composites interleaved with a meltable copolyamide veil},
journal = {Journal of Composite Materials},
year = {2025},
volume = {59},
number = {27},
pages = {3075--3087},
doi = {10.1177/00219983251341631}
}
EUVIMED