EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Effect of TiO 2 and SiC Fillers on the Physical, Mechanical, and Microstructural Characteristics of Hybrid Jute–Flax Fiber–Reinforced Composites

M. Nahid Raihan Jim, Md. Abdul Hasib, Nayan Sur, Bickrom Saha, Arup Kumar Debnath, Md. Sanaul Rabbi, Md. Ashraful Islam

Journal of Engineering · 2026-01 · 2026 (1)

DOI: 10.1155/je/1168825 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Journal of Engineering, online erschienen am 15.11.2026. Verfasst von M. Nahid Raihan Jim und 6 weiteren Autor:innen. Die Arbeit nennt 78 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Hybrid composites incorporating natural fibers are increasingly recognized as environmentally friendly options for lightweight structural components. This study examines the mechanical and microstructural response of epoxy composites reinforced with a five‐layer jute/flax/jute/flax/jute architecture and separately modified with silicon carbide (SiC) or titanium dioxide (TiO 2 ) microparticles. Hand layup laminates were prepared at nominal filler additions of 3%, 5%, and 8% relative to the matrix. Individual additions of SiC and TiO 2 microparticles were made to the epoxy matrix at varying concentrations. Assessment of mechanical properties involved tensile, flexural, impact, and Shore D hardness tests, conducted according to ASTM standards, whereas SEM, XRD, and FTIR analyses were utilized to examine morphology, crystallinity, and chemical interactions. Among the tested formulations, the composite with 3.31 wt.% SiC loading had the highest reported mean tensile strength (50.42 MPa), flexural strength (78.99 MPa), and impact strength (8.58 J/cm 2 ). Its tensile and flexural strengths were approximately 19.5% and 28.2% higher than the control, respectively. The composite with 3.31 wt.% TiO 2 loading had the highest mean tensile and flexural modulus (1 and 4.64 GPa, respectively), whereas the 5.16 wt.% TiO 2 ‐loaded composite had the highest mean Shore D hardness. Strength decreased at the highest nominal loading in both filler series, whereas hardness continued to increase.

Zitieren

APA

Jim, M. N. R., Hasib, M. A., Sur, N., Saha, B., Debnath, A. K., Rabbi, M. S., & Islam, M. A. (2026). Effect of TiO 2 and SiC Fillers on the Physical, Mechanical, and Microstructural Characteristics of Hybrid Jute–Flax Fiber–Reinforced Composites. Journal of Engineering, 2026(1). https://doi.org/10.1155/je/1168825

Vancouver

Jim MNR, Hasib MA, Sur N, Saha B, Debnath AK, Rabbi MS, et al. Effect of TiO 2 and SiC Fillers on the Physical, Mechanical, and Microstructural Characteristics of Hybrid Jute–Flax Fiber–Reinforced Composites. Journal of Engineering. 2026;2026(1). doi:10.1155/je/1168825

BibTeX
@article{Jim2026,
  author = {Jim, M. Nahid Raihan and Hasib, Md. Abdul and Sur, Nayan and Saha, Bickrom and Debnath, Arup Kumar and Rabbi, Md. Sanaul and Islam, Md. Ashraful},
  title = {Effect of TiO 2 and SiC Fillers on the Physical, Mechanical, and Microstructural Characteristics of Hybrid Jute–Flax Fiber–Reinforced Composites},
  journal = {Journal of Engineering},
  year = {2026},
  volume = {2026},
  number = {1},
  doi = {10.1155/je/1168825}
}
Kostenlos starten →