Hydrolytic Degradation and Assessment of Performance of PLA and PBS‐Based Plastics Designed for Packaging Applications

Alberto Lagazzo, Cristina Moliner, Elisabetta Finocchio, Samantha Caputo, Elisabetta Arato

International Journal of Polymer Science · 2025-01 · 2025 (1)

DOI: 10.1155/ijps/5602847 ↗

Kurz gefasst

Fachartikel in der Zeitschrift International Journal of Polymer Science, online erschienen am 25.03.2025. Verfasst von Alberto Lagazzo und 4 weiteren Autor:innen. Die Arbeit wurde bisher 16-mal zitiert (Crossref) und nennt 31 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Horizon 2020 Framework Programme.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Biopolymers based on poly(lactic acid) (PLA) and poly(butylene succinate) (PBS) reinforced with mineral fillers were studied in this work. The mechanical, spectroscopic (FTIR), and morphological (SEM) features of the raw samples were evaluated and compared with those of samples after immersion at diverse temperature (25°C, 37°C, and 70°C) in different degradation mediums (i.e., buffer solutions at pH = 3, 5, and 7.5), simulating their applications as soft and rigid packaging in food containers and cosmetic packaging, respectively. The amount of absorbed water, M s , increased with the increasing temperature as well as the diffusivity, D , indicating faster water diffusion rates. The pH slightly affected M s whereas it produced contrary trends on D : acidic mediums were more aggressive for PLA‐based materials (from 2.2∙10 8 cm 2 /s at pH = 3 to 1∙10 8 cm 2 /s at pH = 7.5 at 25°C) whereas higher pHs resulted in an increase on D for PBS‐based ones (from 1∙10 8 cm 2 /s at pH = 3 to 3.4∙10 8 cm 2 /s at pH = 7.5 at 25°C). The effect of temperature on their mechanical performance, and thus on the aging/degradation of the materials, was predominant, as also evidenced by the morphological analysis, with the pH of the liquid media used to simulate the different packaging applications displaying only a marginal role. FTIR for both PLA and PBS‐based materials indicated that the typical features of the polymers were not significantly changed at the different tested temperatures and no degradation products were detected at pH 3, 5, and 7.5. The obtained results showed the suitability of the PLA and PBS‐based biocomposites for soft and rigid packaging applications where high temperatures are not required for long periods of time. These results will help in the designing of the new improved biocomposites to meet with the target objectives on their applications as packaging materials through the definition of the parameters to be tuned to tailor the bioplastics according to their specific needs.

Förderung

  • Horizon 2020 Framework Programme

Zitieren

APA

Lagazzo, A., Moliner, C., Finocchio, E., Caputo, S., & Arato, E. (2025). Hydrolytic Degradation and Assessment of Performance of PLA and PBS‐Based Plastics Designed for Packaging Applications. International Journal of Polymer Science, 2025(1). https://doi.org/10.1155/ijps/5602847

Vancouver

Lagazzo A, Moliner C, Finocchio E, Caputo S, Arato E. Hydrolytic Degradation and Assessment of Performance of PLA and PBS‐Based Plastics Designed for Packaging Applications. International Journal of Polymer Science. 2025;2025(1). doi:10.1155/ijps/5602847

BibTeX
@article{Lagazzo2025,
  author = {Lagazzo, Alberto and Moliner, Cristina and Finocchio, Elisabetta and Caputo, Samantha and Arato, Elisabetta},
  title = {Hydrolytic Degradation and Assessment of Performance of PLA and PBS‐Based Plastics Designed for Packaging Applications},
  journal = {International Journal of Polymer Science},
  year = {2025},
  volume = {2025},
  number = {1},
  doi = {10.1155/ijps/5602847}
}
Kostenlos starten →