EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Effect of NaOH Concentration, Fiber Length, Fiber Loading, and Filler Loading on the Mechanical Properties of Banana Fiber‐Reinforced Polyester Composites

Lamrot Kebede Kassa, Moera Gutu Jiru, Devendra Kumar Sinha, Satyam Shivam Gautam, Anil Kumar, Akhilesh Kumar Chauhan

Advances in Materials Science and Engineering · 2025-01 · 2025 (1)

DOI: 10.1155/amse/7707280 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Advances in Materials Science and Engineering, online erschienen am 01.07.2025. Verfasst von Lamrot Kebede Kassa und 5 weiteren Autor:innen. Die Arbeit wurde bisher 10-mal zitiert (Crossref) und nennt 55 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

The growing demand for eco‐friendly, lightweight, and high‐performance materials has driven the development of natural fiber‐reinforced polymer composites for use in construction, manufacturing, and automotive applications. However, identifying the optimal fabrication parameters for these composites remains a significant challenge. In this study, polyester‐based composites were fabricated using a simple hand lay‐up method, reinforced with banana fibers and nano alumina (Al 2 O 3 ) powder. Banana fibers of random orientation were used in three lengths (10 mm, 15 mm, and 20 mm) and treated with NaOH solutions at concentrations of 0%, 2.5%, and 5%. A total of nine composite samples were produced by varying the weight percentages of banana fiber (10%, 15%, and 20%) and nano alumina (2 wt%, 4 wt%, and 6 wt%). Gray relational analysis (GRA) was employed to optimize the influence of fiber length, NaOH treatment, fiber content, and filler content on mechanical properties. The optimized composite achieved a tensile strength of 61.7 MPa, a flexural strength of 108.47 MPa, and an impact strength of 19 J at 15 wt% fiber content, 2 wt% nano alumina, 15 mm fiber length, and 5% alkali treatment. The maximum hardness value of 164 HV was recorded for a composite with 20 mm untreated fiber, 15 wt% fiber loading, and 4 wt% nano alumina. The lowest water absorption rate (2.97%) was observed with 10 wt% fiber loading, 6 wt% nano alumina, 20 mm fiber length, and 5% NaOH treatment. These findings contribute to the development of sustainable composite materials, with potential applications in the automotive and aerospace industries.

Zitieren

APA

Kassa, L. K., Jiru, M. G., Sinha, D. K., Gautam, S. S., Kumar, A., & Chauhan, A. K. (2025). Effect of NaOH Concentration, Fiber Length, Fiber Loading, and Filler Loading on the Mechanical Properties of Banana Fiber‐Reinforced Polyester Composites. Advances in Materials Science and Engineering, 2025(1). https://doi.org/10.1155/amse/7707280

Vancouver

Kassa LK, Jiru MG, Sinha DK, Gautam SS, Kumar A, Chauhan AK. Effect of NaOH Concentration, Fiber Length, Fiber Loading, and Filler Loading on the Mechanical Properties of Banana Fiber‐Reinforced Polyester Composites. Advances in Materials Science and Engineering. 2025;2025(1). doi:10.1155/amse/7707280

BibTeX
@article{Kassa2025,
  author = {Kassa, Lamrot Kebede and Jiru, Moera Gutu and Sinha, Devendra Kumar and Gautam, Satyam Shivam and Kumar, Anil and Chauhan, Akhilesh Kumar},
  title = {Effect of NaOH Concentration, Fiber Length, Fiber Loading, and Filler Loading on the Mechanical Properties of Banana Fiber‐Reinforced Polyester Composites},
  journal = {Advances in Materials Science and Engineering},
  year = {2025},
  volume = {2025},
  number = {1},
  doi = {10.1155/amse/7707280}
}
Kostenlos starten →