Influence of Crystallization Time on Energy-Storage Density and Efficiency of Lead-Free Bi 0.5 (Na 0.8 K 0.2 ) 0.5 TiO 3 Thin Films

Ngo Duc Quan, Tran Quoc Toan, Vu Ngoc Hung

Advances in Condensed Matter Physics · 01.01.2019 · 2019 · 1-8

DOI: 10.1155/2019/4949365 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Advances in Condensed Matter Physics, erschienen am 01.01.2019. Verfasst von Ngo Duc Quan und 2 weiteren Autor:innen. Die Arbeit wurde bisher 5-mal zitiert (Crossref) und nennt 34 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: National Foundation for Science and Technology Development.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Lead-free Bi 0.5 (Na 0.80 K 0.20 ) 0.5 TiO 3 (BNKT) ferroelectric films were synthesized on Pt/Ti/SiO 2 /Si substrates via chemical solution deposition. The influence of crystallization time on the microstructures and ferroelectric and energy-storage properties of the films was investigated in detail. The XRD analysis showed that the BNKT films have well crystallized corresponding to the single-phase perovskite structure at 700°C. Ferroelectric and energy-storage properties of the films were significantly enhanced by increasing crystallization time. With crystallization time of 60 min, the remnant polarization ( P r ), maximum polarization ( P m ), and P m - P r values reached the highest values of 7.9 µ C/cm 2 , 28.9 µ C/cm 2 , and 21.0 µ C/cm 2 , respectively, under the electric field of 400 kV/cm. Thanks to the strong enhancement in P m and the large P m a - P r value, the highest recoverable energy-storage density ( J r e c o ) gets the value of 2.9 J/cm 3 . The obtained results indicate that the BNKT films have application potentials in advanced capacitors.

Förderung

  • National Foundation for Science and Technology Development

Zitieren

APA

Quan, N. D., Toan, T. Q., & Hung, V. N. (2019). Influence of Crystallization Time on Energy-Storage Density and Efficiency of Lead-Free Bi 0.5 (Na 0.8 K 0.2 ) 0.5 TiO 3 Thin Films. Advances in Condensed Matter Physics, 2019, 1-8. https://doi.org/10.1155/2019/4949365

Vancouver

Quan ND, Toan TQ, Hung VN. Influence of Crystallization Time on Energy-Storage Density and Efficiency of Lead-Free Bi 0.5 (Na 0.8 K 0.2 ) 0.5 TiO 3 Thin Films. Advances in Condensed Matter Physics. 2019;2019:1-8. doi:10.1155/2019/4949365

BibTeX
@article{Quan2019,
  author = {Quan, Ngo Duc and Toan, Tran Quoc and Hung, Vu Ngoc},
  title = {Influence of Crystallization Time on Energy-Storage Density and Efficiency of Lead-Free Bi 0.5 (Na 0.8 K 0.2 ) 0.5 TiO 3 Thin Films},
  journal = {Advances in Condensed Matter Physics},
  year = {2019},
  volume = {2019},
  pages = {1--8},
  doi = {10.1155/2019/4949365}
}
Kostenlos starten →