Anomalously Faster Deterioration of LiNi 0.8 Co 0.15 Al 0.05 O 2 /Graphite High-Energy 18650 Cells at 1.5 C than 2.0 C

Dawei Cui iD, Jinlong Wang iD, Ailing Sun iD, Hongmei Song iD, Wenqing Wei iD

Scanning · 31.07.2018 · 2018 · 1-7

DOI: 10.1155/2018/2593780 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Scanning, erschienen am 31.07.2018. Verfasst von Dawei Cui und 4 weiteren Autor:innen. Beteiligte Einrichtung: School of Mechanical-Electronic and Vehicle Engineering, Weifang University, Weifang 261061, China. Die Arbeit wurde bisher 6-mal zitiert (Crossref) und nennt 33 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: National Natural Science Foundation of China, Distinguished Middle-Aged and Young Scientist Encourage and Reward Foundation of Shandong Province, Natural Science Foundation of Shandong Province.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Discharge rate is a key parameter affecting the cycle life of lithium-ion batteries (LIB). Normally, lithium-ion batteries deteriorate more severely at a higher discharge rate. In this paper, we report that the cycle performance of LiNi 0.8 Co 0.15 Al 0.05 O 2 /graphite high-energy 2.8 Ah 18650 cells is abnormally worse at a 1.5 C discharge rate than at a 2.0 C discharge rate. Combining macromethods with micromethods, the capacity/rate performance, electrochemical impedance spectroscopy (EIS), and scanning electron microscope (SEM) morphology of the electrodes are systematically investigated. We have found that the impedance of the negative electrodes after 2.0 C aged is smaller than that after 1.5 C aged, through EIS analysis, and the discharge rate performance of the negative electrodes after 2.0 C aged is better than that after 1.5 C aged through coin cell analysis. In addition, some special microcracks in the negative electrodes of aged cells are observed through SEM analysis, which can accelerate the side reaction between active and electrolyte and form the thicker SEI which will hinder the Li + insertion and cause resistance increase. In short, the LiNi 0.8 Co 0.15 Al 0.05 O 2 /graphite-based lithium-ion batteries show better cycle life at a 2.0 C discharge rate than at a 1.5 C discharge rate which indicates that the negative electrodes contribute more than the positive electrodes.

Autor:innen und Institutionen

  • School of Mechanical-Electronic and Vehicle Engineering, Weifang University, Weifang 261061, China.

ORCID-Profile: Dawei Cui, Jinlong Wang, Ailing Sun, Hongmei Song, Wenqing Wei

Förderung

  • National Natural Science Foundation of China
  • Distinguished Middle-Aged and Young Scientist Encourage and Reward Foundation of Shandong Province
  • Natural Science Foundation of Shandong Province

Zitieren

APA

Cui, D., Wang, J., Sun, A., Song, H., & Wei, W. (2018). Anomalously Faster Deterioration of LiNi 0.8 Co 0.15 Al 0.05 O 2 /Graphite High-Energy 18650 Cells at 1.5 C than 2.0 C. Scanning, 2018, 1-7. https://doi.org/10.1155/2018/2593780

Vancouver

Cui D, Wang J, Sun A, Song H, Wei W. Anomalously Faster Deterioration of LiNi 0.8 Co 0.15 Al 0.05 O 2 /Graphite High-Energy 18650 Cells at 1.5 C than 2.0 C. Scanning. 2018;2018:1-7. doi:10.1155/2018/2593780

BibTeX
@article{Cui2018,
  author = {Cui, Dawei and Wang, Jinlong and Sun, Ailing and Song, Hongmei and Wei, Wenqing},
  title = {Anomalously Faster Deterioration of LiNi 0.8 Co 0.15 Al 0.05 O 2 /Graphite High-Energy 18650 Cells at 1.5 C than 2.0 C},
  journal = {Scanning},
  year = {2018},
  volume = {2018},
  pages = {1--7},
  doi = {10.1155/2018/2593780}
}
Kostenlos starten →