Solid-Gas Interphase Formation in Anode-Free Solid-State Batteries
ECS Meeting Abstracts · 07.07.2026 · MA2026-01 (4) · 535-535
DOI: 10.1149/ma2026-014535mtgabs ↗Kurz gefasst
Fachartikel in der Zeitschrift ECS Meeting Abstracts, erschienen am 07.07.2026. Verfasst von Ryosuke Iwamura und 10 weiteren Autor:innen.
Abstract (Originalsprache)
Solid-state batteries paired with Li metal anodes offer the potential for high energy density. However, due to the high reactivity of Li metal, undesirable side reactions can occur at the solid electrolyte interface. The solid electrolyte interphase (SEI), contributes to stabilizing the interface between the Li metal and the solid electrolyte. In addition to these reactions with the electrolyte, Li metal also reacts with the ambient gas, and its byproduct affects the Coulombic efficiency. In liquid Li metal batteries, electrodes are fully wetted by the liquid electrolyte, which minimizes other side reactions. In contrast, there is no liquid electrolyte, and trace amount of gas exist in solid-state batteries. Most commercial Li ion batteries are produced in dry rooms and sealed under rough vacuum pressures, meaning that small amounts of nitrogen, oxygen, and carbon dioxide remain within the cell. In this work, we study the dynamic formation of a solid gas interphase (SGI) layer on the exposed surfaces of the Li metal anode during plating, stripping, and open-circuit rest periods [1]. A customized environmental chamber was manufactured to allow for precise control of the background gas composition and pressure while cycling SSBs under stack pressure. The formation of an SGI was found to depend on the plated Li capacity, ambient gas composition, and aging time, which has a direct impact on Coulombic efficiency. Under a gas environment with elevated nitrogen levels, Coulombic efficiency significantly decreased. Optical observations of the anode electrolyte surface revealed the presence of residual phases that are attributed to the formation of an SGI through reactions with nitrogen. To reveal the dynamic formation of the SGI layer with trace background reactant gases, operando x-ray photoelectron spectroscopy (XPS) was performed under ultra-high vacuum conditions. These results indicate that even under high-vacuum conditions, Li metal can react with residual nitrogen and oxygen to form an SGI. Solid-state pouch cells were assembled in a commercially relevant dry room environment, revealing the influence of SGI formation on calendar life in practical cell configurations. These findings highlight the importance of SGI formation, which is distinct from the classical SEI layer that arises from electrolyte decomposition, in the analysis of SSBs. [1]D. W. Liao, D. Zeng, G. K. Mishra, S. Y. Lee, A. M. Melemed, D. Penley, R. Iwamura, H. Kawakami, Y. Aihara, K. Aotani, N. P. Dasgupta, “Solid-Gas Interphase Formation in Anode-Free Solid-State Batteries”, J. Am. Chem. Soc., In Press (2025).
Zitieren
APA
Iwamura, R., Liao, D. W., Zeng, D., Mishra, G. K., Lee, S. Y., Melemed, A. M., Penley, D., Kawakami, H., Aihara, Y., Aotani, K., & Dasgupta, N. P. (2026). Solid-Gas Interphase Formation in Anode-Free Solid-State Batteries. ECS Meeting Abstracts, MA2026-01(4), 535-535. https://doi.org/10.1149/ma2026-014535mtgabs
Vancouver
Iwamura R, Liao DW, Zeng D, Mishra GK, Lee SY, Melemed AM, et al. Solid-Gas Interphase Formation in Anode-Free Solid-State Batteries. ECS Meeting Abstracts. 2026;MA2026-01(4):535-535. doi:10.1149/ma2026-014535mtgabs
BibTeX
@article{Iwamura2026,
author = {Iwamura, Ryosuke and Liao, Daniel W. and Zeng, Davy and Mishra, Govind K and Lee, Si Young and Melemed, Aaron Max and Penley, Daniel and Kawakami, Hiroki and Aihara, Yuichi and Aotani, Koichiro and Dasgupta, Neil P.},
title = {Solid-Gas Interphase Formation in Anode-Free Solid-State Batteries},
journal = {ECS Meeting Abstracts},
year = {2026},
volume = {MA2026-01},
number = {4},
pages = {535--535},
doi = {10.1149/ma2026-014535mtgabs}
}
EUVIMED