Effect of Hydration on Electrical Properties of Lanthanum-Cerium Oxides

Or Ben Zion, David Ehre, Alexey Rulev, Vladimir Pomjakushin, Artur Braun, Isaac Abrahams, Igor Lubomirsky

ECS Meeting Abstracts · 07.07.2026 · MA2026-01 (39) · 2018-2018

DOI: 10.1149/ma2026-01392018mtgabs ↗

Kurz gefasst

Fachartikel in der Zeitschrift ECS Meeting Abstracts, erschienen am 07.07.2026. Verfasst von Or Ben Zion und 6 weiteren Autor:innen.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

With the goal of developing a technologically friendly, water- and CO₂-stable ceramic proton conductor operating below 473 K, we have investigated the hydration of La x Ce 1-x O 2-x/2 (LCO). We found that for x > 0.5, it decomposes to La(OH) 3 and CeO 2 upon contact with water or water vapor. For x < 0.4, no hydration was achieved during exposure to 1 atm steam for >14 days, limiting our investigation to LCO40, LCO45, and LCO50. Exposure of LCO50 ceramics to P H 2O =1 atm at 200 °C leads to a maximum hydration of f h =4.4 ±0.2%. For other compositions, the degree of hydration at this pressure is even lower. For all compositions, hydration causes lattice expansion, leading to near-surface shear stress and subsequent cracking, which prevents electrical and mechanical measurements. Increasing the temperature at P H 2O =1 atm, alleviates cracking due to increased vacancy mobility but does not increase fₕ , because dehydration occurs above 350 °C. To address this problem, we have developed a hydration chamber (pressure vessel) in which water is introduced and controlled by the decomposition of CoSO 4 ·7H 2 O. This method does not allow independent control of pressure and temperature but sets a unique dependence between them via the thermodynamics of CoSO 4 ·7H 2 O dehydration. At 400 °C and P H 2O =56 ±3 atm , hydration of LCO50 still poses a problem because the high P H 2O drives the material close to decomposition, even though relative lattice expansion Δd/d> 0.5% can be achieved. For LCO40, Δd/d< 0.1% and fₕ 0.43 and fₕ >38.5%. Surprisingly, the latter is the maximum possible achievable at these conditions irrespective of the exposure time 5-120 hrs. The volume per mol water absorbed drops by a factor of three in the range fₕ =0-38.5% suggesting some long-range proton interactions. Hydration causes an approximately 10–40-fold increase in electrical conductivity in the range 383–483 K. However, even if the conductivity is proton-dominated, the activation energy remains ~0.8 eV, about twice that of doped BaZrO₃ proton conductors. Although hydrated LCO45 and BaZrO₃ have similar proton concentrations and oxygen–oxygen distances, the proton mobility in LCO45 is 100 times lower. Hydration does not affect the elastic or electrostrictive properties of LCO, suggesting that protons interact with only one oxygen ion at a time and can freely reorient around it. Preliminary neutron diffraction data support this interpretation and indicate possible strategies for improving conductivity.

Zitieren

APA

Zion, O. B., Ehre, D., Rulev, A., Pomjakushin, V., Braun, A., Abrahams, I., & Lubomirsky, I. (2026). Effect of Hydration on Electrical Properties of Lanthanum-Cerium Oxides. ECS Meeting Abstracts, MA2026-01(39), 2018-2018. https://doi.org/10.1149/ma2026-01392018mtgabs

Vancouver

Zion OB, Ehre D, Rulev A, Pomjakushin V, Braun A, Abrahams I, et al. Effect of Hydration on Electrical Properties of Lanthanum-Cerium Oxides. ECS Meeting Abstracts. 2026;MA2026-01(39):2018-2018. doi:10.1149/ma2026-01392018mtgabs

BibTeX
@article{Zion2026,
  author = {Zion, Or Ben and Ehre, David and Rulev, Alexey and Pomjakushin, Vladimir and Braun, Artur and Abrahams, Isaac and Lubomirsky, Igor},
  title = {Effect of Hydration on Electrical Properties of Lanthanum-Cerium Oxides},
  journal = {ECS Meeting Abstracts},
  year = {2026},
  volume = {MA2026-01},
  number = {39},
  pages = {2018--2018},
  doi = {10.1149/ma2026-01392018mtgabs}
}
Kostenlos starten →