EUVIMEDEUVIMED entdecken
Crossref

In-Situ Grazing-Incidence X-Ray Absorption Spectroscopy of MnO 2 Cathode Interfaces in Zinc-Ion Batteries

Wathanyu Kao-ian, Soorathep Kheawhom

ECS Meeting Abstracts · 07.07.2026 · MA2026-01 (3) · 512-512

DOI: 10.1149/ma2026-013512mtgabs ↗

Kurz gefasst

Fachartikel in der Zeitschrift ECS Meeting Abstracts, erschienen am 07.07.2026. Verfasst von Wathanyu Kao-ian und 1 weiteren Autor:innen.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Rechargeable zinc-ion batteries (ZIBs) have emerged as a promising alternative to lithium-based systems for large-scale and stationary energy storage due to their intrinsic safety, low cost, and the natural abundance of zinc. Among various cathode candidates, manganese dioxide (MnO 2 ) is particularly attractive because of its high theoretical capacity and environmental benignity. However, despite extensive research efforts, MnO 2 -based ZIBs continue to suffer from limited rate capability and progressive capacity fading during cycling. These performance limitations are increasingly attributed to complex and poorly understood interfacial processes occurring at the cathode–electrolyte boundary, especially under deep discharge and prolonged cycling. Conventional ex-situ characterization and bulk-averaged operando techniques often fail to capture such surface-localized phenomena, obscuring their mechanistic role in cathode degradation. In this work, we present the first application of i n-situ grazing-incidence X-ray absorption spectroscopy (GI-XAS) to directly probe depth-dependent redox and structural dynamics at the MnO 2 cathode interface during the operation of a zinc-ion battery. By combining a custom-designed electrochemical cell with synchrotron-based Mn K-edge XANES measurements, we achieve real-time, element-specific insight into the chemical evolution of Mn at both the near-surface interfacial region and the bulk of the cathode. The grazing-incidence geometry allows the X-ray penetration depth to be tuned from a few nanometers to several micrometers simply by adjusting the incident angle, enabling a direct comparison between surface-sensitive and bulk-sensitive responses under identical electrochemical conditions. The study focuses on a layered δ-MnO 2 (birnessite) cathode operating in a hybrid “wet” nonaqueous electrolyte composed of Zn 2+ salt dissolved in dimethylformamide with a small water additive. Bulk-sensitive GI-XAS measurements reveal that the MnO₂ cathode undergoes a largely reversible Mn⁴⁺/Mn³⁺ redox process during Zn 2+ insertion and extraction, with the Mn K-edge position returning close to its original state upon full recharge. This observation suggests that, when averaged across the electrode thickness, the cathode appears electrochemically reversible, consistent with conclusions drawn from conventional bulk operando probes and electrochemical profiles. In sharp contrast, surface-sensitive GI-XAS uncovers a distinctly different interfacial behavior. At deep discharge, the Mn K-edge XANES spectra collected at grazing incidence show a pronounced shift toward lower energies, accompanied by spectral features characteristic of Mn 2+ species. Simultaneously, a substantial increase in Mn fluorescence intensity is observed, indicating the formation of Mn 2+ -rich species at or near the cathode surface. These results provide direct evidence that MnO 2 undergoes interfacial reduction beyond Mn 3+ to Mn 2+ , consistent with a dissolution mechanism in which Mn is released into the electrolyte at the cathode–electrolyte interface. Upon subsequent charging, the surface Mn 2+ species do not immediately reintegrate into the original MnO 2 lattice. Instead, GI-XAS reveals the formation of a transient Mn-rich interfacial layer during the early stages of charge, which correlates with an increased overpotential in the electrochemical response. As charging proceeds, this layer partially re-oxidizes toward higher Mn valence states; however, even after full recharge, the surface spectra do not completely recover to the pristine Mn 4+ state. Residual Mn 2+ /Mn 3+ species persist at the interface, indicating incomplete reversibility of the surface reconstruction process. Electrochemical impedance spectroscopy further confirms a progressive increase in charge-transfer resistance upon cycling, consistent with the accumulation of an interfacial passivation layer. These findings demonstrate that cathode degradation in Zn–MnO 2 batteries is governed not by bulk redox failure, but by surface-specific dissolution–redeposition and incomplete reoxidation of Mn species, which gradually impede Zn 2+ transport and electron transfer. Crucially, such interfacial mechanisms are invisible to bulk-averaged operando techniques and can only be resolved using depth-sensitive probes such as GI-XAS. Beyond elucidating the degradation pathway of MnO 2 cathodes, this work establishes in-situ GI-XAS as a powerful and generalizable operando methodology for studying solid–liquid interfaces in electrochemical energy storage systems. The approach provides unique, chemically specific insight into interfacial redox processes that dictate long-term performance and failure. These insights offer a rational foundation for the development of interface-stabilization strategies, including electrolyte engineering, surface coatings, and Mn-chelation approaches, aimed at improving the durability and rate capability of next-generation zinc-based batteries.

Zitieren

APA

Kao-ian, W., & Kheawhom, S. (2026). In-Situ Grazing-Incidence X-Ray Absorption Spectroscopy of MnO 2 Cathode Interfaces in Zinc-Ion Batteries. ECS Meeting Abstracts, MA2026-01(3), 512-512. https://doi.org/10.1149/ma2026-013512mtgabs

Vancouver

Kao-ian W, Kheawhom S. In-Situ Grazing-Incidence X-Ray Absorption Spectroscopy of MnO 2 Cathode Interfaces in Zinc-Ion Batteries. ECS Meeting Abstracts. 2026;MA2026-01(3):512-512. doi:10.1149/ma2026-013512mtgabs

BibTeX
@article{Kaoian2026,
  author = {Kao-ian, Wathanyu and Kheawhom, Soorathep},
  title = {In-Situ Grazing-Incidence X-Ray Absorption Spectroscopy of MnO 2 Cathode Interfaces in Zinc-Ion Batteries},
  journal = {ECS Meeting Abstracts},
  year = {2026},
  volume = {MA2026-01},
  number = {3},
  pages = {512--512},
  doi = {10.1149/ma2026-013512mtgabs}
}
Kostenlos starten →