( Invited ) Controlling Plating and Stripping Processes Along Lithium/Solid Electrolyte Interfaces
ECS Meeting Abstracts · 07.07.2026 · MA2026-01 (3) · 370-370
DOI: 10.1149/ma2026-013370mtgabs ↗Kurz gefasst
Fachartikel in der Zeitschrift ECS Meeting Abstracts, erschienen am 07.07.2026. Verfasst von Neil P. Dasgupta.
Abstract (Originalsprache)
Solid-state batteries have the potential to transform electrochemical energy storage technology by replacing the liquid electrolytes typically used in rechargeable batteries with a solid-state electrolyte. The use of a solid electrolyte can potentially improve battery safety, and may also enable higher energy densities through the use of an alkali metal (Li, Na) anode. However, when a liquid electrolyte is replaced by a solid phase, the interfacial processes that occur during charging and discharging are governed by different physico-chemical processes [1]. In this talk, I will summarize recent findings in understanding and controlling the electrodeposition (plating) and dissolution (stripping) processes that occur along the interface between a Li metal anode and a ceramic solid electrolyte during cycling. During charging of the battery, Li plating occurs through a series of nucleation and growth processes [1]. In particular, the nature of the electronically conducting phase (e.g. current collector, metal anode, and/or interlayer) can substantially modify the energy landscape during the plating process. In this talk, I will focus on understanding nucleation and growth phenomena with, and without, reactive interlayer materials along the interface. The role of spatial heterogeneity will be described, including influences of both chemical and mechanical factors [2-4]. During discharge, I will describe the depletion of Li metal along the interface, with a particular focus on mechanisms of electrical contact loss (e.g. void formation) [5]. The ability to measure contact loss during stripping will be described using a combination of in situ/operando probes, and strategies to minimize and reverse void formation will be described. References [1] A. J. Sanchez, N. P. Dasgupta, J. Am. Chem. Soc. 146 , 4282 (2024) [2] D. W. Liao, D. Zeng, M. Mulla, A. Madanchi, H. Kawakami, Y. Aihara, K. Aotani, M. D. Thouless, N. P. Dasgupta, Adv. Mater. 37 , 2502114 (2025) [3] M. A. Thorpe, M. Zhang, D. W. Liao, S. E. Sandoval, Y. Kim, M. T. McDowell, M. D. Thouless, N. P. Dasgupta, Matter 8 , 101955 (2025) [4] J. S. Yoon, D. W. Liao, S. M. Greene, T. H. Cho, N. P. Dasgupta, D. J. Siegel, ACS Appl. Mater. Interfaces 16 , 18790 (2024) [5] K. Lee, E. Kazyak, M. J. Wang, N. P. Dasgupta, J. Sakamoto, Joule 6 , 2547 (2022)
Zitieren
APA
Dasgupta, N. P. (2026). ( Invited ) Controlling Plating and Stripping Processes Along Lithium/Solid Electrolyte Interfaces. ECS Meeting Abstracts, MA2026-01(3), 370-370. https://doi.org/10.1149/ma2026-013370mtgabs
Vancouver
Dasgupta NP. ( Invited ) Controlling Plating and Stripping Processes Along Lithium/Solid Electrolyte Interfaces. ECS Meeting Abstracts. 2026;MA2026-01(3):370-370. doi:10.1149/ma2026-013370mtgabs
BibTeX
@article{Dasgupta2026,
author = {Dasgupta, Neil P.},
title = {( Invited ) Controlling Plating and Stripping Processes Along Lithium/Solid Electrolyte Interfaces},
journal = {ECS Meeting Abstracts},
year = {2026},
volume = {MA2026-01},
number = {3},
pages = {370--370},
doi = {10.1149/ma2026-013370mtgabs}
}
EUVIMED